ALPHA 3355-11

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA 3355-11

Main features

  • VOC-Free Water-Soluble Fluxing
  • Flexible Multi-Method Application
  • Thorough Water-Residue Removal

Product Description

ALPHA 3355-11 Water Soluble Flux is a VOC-free, water-soluble organic-acid liquid soldering flux for printed circuits and electronic hardware. It supports foam, spray, dip, wave, and brush application, allowing the fluxing method to match the assembly line. Flux applicators and reservoirs should use plastic or titanium construction. Preheat is adjusted for conveyor speed, component type, and substrate, with a topside temperature near 210 deg F on entry to the solder wave identified as typical. Its water-soluble post-solder residues are intended for thorough removal after soldering.

Key features

  • VOC-free organic-acid flux: The water-soluble liquid formulation supports soldering processes that specify a VOC-free flux.
  • Multiple application methods: Foam, spray, dip, wave, and brush options provide flexibility across printed-circuit soldering equipment.
  • Water-removable residues: Water-soluble residues are designed for thorough post-solder removal from electronic hardware.

Applications

Applications include soldering printed circuits and electronic hardware by foam, spray, dip, wave, or brush flux application.

Product Family

ALPHA 3355-11

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
17 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.950 ± 0.020 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Use plastic or titanium for flux applicators and reservoirs.

PropertyValueUnitMethod / condition
FormLiquidAs supplied
Flux typeWater-soluble organic acidAs supplied
VOC contentVOC-freeAs supplied
Application methodsFoam, spray, dip, wave, or brushBefore soldering