ALPHA 2110

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA 2110

Main features

  • Aqueous Rosin Residue Removal
  • Multiple Cleaning Equipment Formats
  • Stable Silicone-Free Wash Solution

Product Description

ALPHA 2110 Electronic Cleaner is a concentrated aqueous saponifier for removing rosin flux residues from printed circuit boards and electronics assemblies. It is used at 3 to 5 vol% in conveyorized equipment, 4 to 8 vol% in soak tanks, 2 to 3 vol% in modified dishwashers, and 10 vol% for reflowed rosin-paste residues. Recommended wash temperature is 150 to 160 deg F. The buffered cleaner maintains solution composition during recirculation and operates without silicone defoamers. Wetted equipment parts should not use polycarbonate, Viton, neoprene, natural rubber, copper, aluminum, brass, or galvanized metal.

Key features

  • Aqueous rosin-residue cleaning: Converts rosin residues into water-soluble soaps for removal from printed circuit assemblies.
  • Equipment-specific concentration ranges: Defined use levels cover conveyorized machines, soak tanks, modified dishwashers, and reflow-paste residues.
  • Recirculated solution stability: Maintains composition during prolonged recirculation and operates without silicone defoamers.

Applications

Applications include removing rosin flux residues from printed circuit boards and electronics assemblies in conveyorized machines, soak tanks, and modified dishwashers.

Product Family

ALPHA 2110

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Aqueous rosin cleaner / saponifier
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.001 ± 0.005 @ 25°C
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
99 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Concentrations are by volume for the cleaner concentrate; the appropriate level depends on throughput, wash time, and contamination load.

PropertyValueUnitMethod / condition
Specific gravity1.001 +/- 0.00525 deg C
pH11.65 vol% solution
Flash point99deg CCleveland Open Cup
Recommended concentration, conveyorized3 to 5vol%Wash solution
Recommended concentration, soak tank4 to 8vol%Wash solution
Recommended concentration, modified dishwasher2 to 3vol%Wash solution
Recommended concentration, reflowed rosin-paste residue10vol%Wash solution
Recommended wash temperature150 to 160deg FTypical wash tank