Aculon FS - 3 Series Extender

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Aculon FS - 3 Series Extender Aculon FS - 3 Series Extender Aculon FS - 3 Series Extender

Main features

  • Fluorinated Solvent
  • Clear material
  • 3M Novec 7100 alternative

Product Description

Aculon FS - 3 Series Extender is a fluorinated solvent used for cleaning, diluting, and as a carrier solvent for several of Aculon’s branded products. It is a direct alternative to 3M NOVEC 7100.

Aculon FS - 3 has excellent compatibility with multiple materials such as ABS, EPDM, Fluoroelastomers, Polypropylene, PTFE and other. You can find more in the additional information section.

Product Family

ACULON NanoProof 3-FSE

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.5
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1 mPa.s

Additional Information

Aculon FS3 Extender vs 3M Novec 7100

  3M Novec 7100 Aculon FS 3 Series Extender
Viscosity <5 cP <1 cP
Boiling point 61°C 56-61°C
Freezing point -135°C -81°C
Flash point None None
Specific gravity 1.52 g/mL 1.5 g/mL
Shelf life 2 years (unopened container) 2 years (unopened container)

Aculon 3 Series Extender has been accepted for commercial use by regulatory agencies in the U.S, E.U and China.
Aculon 3 Series Extender has been excluded by the U.S. EPA from the definition of a VOC on the basis that this compound has a negligible contribution to tropospheric ozone formation.

 

Compatibility

Material Compatibility
ABS

At boiling point for 3 days, <0.1% Weight change, <0.1% Linear swell

EPDM

At boiling point for 3 days, <0.1% Weight change, <0.1% Linear swell

Fluorelastomer

At boiling point for 3 days, >86% Weight change, >24% Linear swell

Polymethyl methacrylate At boiling point for 3 days, affected, affected
Polypropylene

At boiling point for 3 days, <2.5% Weight change, <1% Linear swell

Polysterene

At boiling point for 3 days, <0.1% Weight change, <0.1% Linear swell

PTFE

At boiling point for 3 days, <2.5% Weight change, <0.1% Linear swell

Silicone Rubber

At boiling point for 3 days, <12.5% Weight change, <2.5% Linear swell

Leading Brands Trust in Our Products and Services