Aculon Nanoproof 3-001X

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Aculon Nanoproof 3-001X Aculon Nanoproof 3-001X Aculon Nanoproof 3-001X Aculon Nanoproof 3-001X

Main features

  • 0.1% Fluoroacrylate Solids
  • 1 um Thickness
  • 3M Novec 1720 replacement

Product Description

Aculon Nanoproof 3-001X is a highly effective electronic coating series designed to provide superior protection against moisture, chemicals, and corrosion for a wide range of electronic applications. With the discontinuation of the popular 3M Novec product line, the Aculon Nanoproof 3.0 series offers a readily available and accessible alternative for industries that require robust protection for their electronic devices.

Aculon Nanoproof 3-001X with 0.1% Fluoroacrylate solids, forms a thin, transparent layer that provides excellent anti-wetting and anti-stiction properties, protecting LED devices from harmful elements. With this amount of solids, it manages to reach a coating thickness of less than 1um. The coating also offers electrical insulation properties, reducing the risk of electrical shorts and failures of PCBs and Electrical components.

The Aculon Nanoproof 3.0 series comes in different grades, with Aculon Nanoproof 3-001X allowing such a thin coating that is adirect alternative to 3M 1720 Novec products It is ideal for use in harsh environments, making it a popular choice in industries such as automotive, aerospace, and defense. Aculon Nanoproof 3-001X is easy to apply, and its transparent coating ensures that it does not interfere with the aesthetics or functionality of electronic devices. It is suitable for use on a variety of electronic applications, including printed circuit boards, sensors, switches, and connectors.

Applications:

  • Moisture, chemical, and corrosion protection for printed circuit boards and electrical components
  • Anti-wetting and anti-stiction in many diverse applications
Product Family

ACULON NanoProof 3-001X

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.376
Solids
0.1 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
95 °C
Other Properties
Oil Contact Angle
The contact angle is the angle, conventionally measure trough the liquid, where a liquid-vapor interface meets a solid surface.
80 °
Water Contact Angle
120 °

Additional Information

Thickness depends on the amount of Solids. The higher the amount of solids, the thicker the coating after the solvent evaporates.

 

Aculon Nanoproof 3-001X vs 3M Novec 1720

  3M Novec 1720 Aculon Nanoproof 3-001X
Solids Fluoroacrylate 0.1% Fluoroacrylate 0.1%
Solvent 7100DL 3 Series Extender
Appearance Clear Clear
Density 1.5 g/ml 1.5 g/ml
Viscosity <20 cP <20 cP
Boiling point 61°C 56-61°C
Environmental Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine
Shelf life 2 years 2 years
Thickness <1 um <1 um
Tg -110°C 95°C
Thermal Stability of dry film 200°C om air >3h In process
Contact angles WCA/OCA: 105°/65° WCA/OCA: 120°/80°
Refractive Index 1.39 1.376
Solder through repairability Yes Yes
Cure 135°C for 15 minutes None
Application Anti stiction, Chemical protection, Corrosion protection, Moisture protection Anti stiction, Chemical protection, Corrosion protection, Moisture protection