Aculon 73DE Offset

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Aculon 73DE Offset

Main features

  • Fluorinated Solvent
  • Heavy duty vapor degrease
  • 3M Novec 73DE alternative

Product Description

Aculon 73DE Offset is a clear fluorinated solvent blend designed for heavy-duty vapor degreasing or immersion cleaning applications. Some of the features include high solvency, low surface tension, non-flammability, and fluid stability.

Vapor degreasing with Aculon 73DE fluid can help save time and costs over by offering faster cycle times, lower energy usage, and improved cleaning of parts with complex geometries. It is a direct replacement for Novec 73DE.

 

Key Features

  • Effective in cleaning heavy greases, oils, waxes, silicones, and non-polar flux residues.
  • Easy maintenance and use in a vapor degreaser with stable bath composition during extended use.
  • Non-flammable and low in toxicity.
  • Environmentally sustainable with low global warming potential (GWP) and 0 ozone depletion potential(ODP).
  • Replacement for Novec 73DE, nPB, TCE, ozone-depleting HCFCs, and high GWP HFCs.
  • Effective for lubricant deposition applications where increased solvency is desired.
Product Family

ACULON 73DE-OFF

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
clear/colorless
Solids
none %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.28
Vapor Pressure
0.36 kg/cm2
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
48 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1 mPa.s

Additional Information

Aculon 73DE Offset vs 3M Novec 73DE

  3M Novec 73DE Aculon 73DE
Viscosity (cP) 0.38 cP <1 cP
Liquid Density (g/mL) 1.28 1.28
Boiling point (°C) 48  48 
Surface Tension (dynes/cm) 19.9 19.9
Kauri-Butanol Value 83 83
Vapor Pressure (mm/Hg @ 20 °C) 263 263
Heat of Vaporization
(cal/g @ boiling point)
54.2 54.2
Shelf life 2 years 2 years

 

 

Aerospace Materials Compatibility

Test Description ASTM Method Test result
Sandwich Corrosion F1110  Passes
Effect on Painted Surfaces F502 Passes
Hydrogen Embrittlement F519  Passes
Effect on Unpainted Surfaces F485  Passes
Total Immersion Corrosion F483 Passes
Low-Embrittling Cadmium Plate F1111 Passes
Flash Point  D56  Passes
Acrylic Stress Crazing F484  Does Not Pass
Stress Corrosion of Titanium Alloys  F945  Passes

 

 

 

Compatibility with Materials

Plastics Compatible Acetal, Epoxy, Nylon, PEEK, Polyester, Polyethylene, Polypropylene, PTFE
Plastics Incompatible ABS, Polystyrene, Acrylic, Polycarbonate
Elastomers Compatible DuPont Kalrez Perfluoroelastomers, Butyl Rubber, Parfluor Perfluoroelastomers,
Viton Fluoroelastomers, Polyurethane
Elastomers Incompatible Silicone, Fluorosilicone
Metals Compatible Copper, Brass, Stainless Steel, Magnesium, Titanium, Aluminum, Carbon Steel,