ABLESTIK ECF 568

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK ECF 568

Main features

  • Electrically Conductive Application
  • 2-Hour 95 deg C Cure
  • Sheet Stock or Die-Cut Preforms

Product Description

LOCTITE® ABLESTIK ECF 568 is a high-purity, electrically conductive epoxy film adhesive designed for substrate-attach applications. The silver film uses a glass-fabric carrier with a nominal carrier thickness of 1 mil and is supplied as sheet stock or customer-specific die-cut preforms. It provides a typical 24-hour work life at 25°C and heat-cure options of 2 hours at 95°C or 4 hours at 75°C. Cured performance includes electrical resistance of 0.002 ohm per 0.5 in² measured through gold joints and lap shear strength of 3,500 psi for gold-to-gold bonds at 25°C.

Key features

  • Electrically conductive film: Typical electrical resistance is 0.002 ohm per 0.5 in² when measured through cured gold joints.
  • Low-temperature heat cure: Guideline cure schedules include 2 hours at 95°C or 4 hours at 75°C.
  • Preformed adhesive format: Available as sheet stock or die-cut preforms for substrate-attach assembly.

Applications / Suitable for

  • Substrate-attach applications
  • Electrically conductive bonding through gold joints
  • Assembly processes using sheet stock or die-cut adhesive preforms

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Silver
Chemistry Type
Epoxy Film
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
113 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, handling, storage, and cure information for the adhesive film before final processing.

Property Value Unit Method / condition
Technology Epoxy film — As supplied
Appearance Silver film — Solid film
Carrier type Glass fabric — Adhesive-film construction
Carrier thickness 1 mil Nominal carrier thickness
Work life 24 hours At 25°C
Shelf life 365 days At -40°C, from date of manufacture
Cure schedule 2 hours or 4 hours — 2 hours at 95°C or 4 hours at 75°C; maintain 2–10 psi pressure during cure
Technical properties

After-processing / final-state properties

Typical cured-film properties and bonded-joint performance. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Coefficient of thermal expansion — below Tg 65 ppm/°C TMA; cure condition not stated
Coefficient of thermal expansion — above Tg 400 ppm/°C TMA; cure condition not stated
Glass-transition temperature 113 °C TMA; cure condition not stated
Electrical resistance through gold joints 0.002 ohm/0.5 in² Measured through gold joints
Lap shear strength — aluminum to aluminum 5,100 psi Tested at 25°C; aluminum surface condition and cure condition not stated
Lap shear strength — gold to gold 3,500 psi Tested at 25°C; surface preparation and cure condition not stated