ABLESTIK 9392

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK 9392

Main features

  • Flexible Cured Adhesive
  • 168-Hour 24 deg C Cure
  • 1.00 x 10^13 ohm-cm Volume Resistivity

Product Description

LOCTITE ABLESTIK 9392 is a clear amber, two-component epoxy encapsulant designed for general potting applications. The mixed material has a typical viscosity of 17,000 mPa.s (cP) and a specific gravity of 1.0. It can be cured at room temperature or with heat, using guideline schedules of 168 hours at 24 degC or 16 hours at 82 degC. The cured material is flexible and provides documented electrical insulation, shear strength, and tensile strength.

Key Features

  • Two-component epoxy encapsulant for general potting applications
  • Clear amber appearance
  • Room-temperature or heat-cure capability
  • Typical mixed viscosity of 17,000 mPa.s (cP)
  • Flexible cured material with Shore A hardness of 60
  • Typical cured volume resistivity of 1.00 x 10^13 ohm-cm at 25 degC

Applications / Suitable for

  • General potting and encapsulation
  • Assemblies involving metals, wood, many plastics, and rubber
  • Applications requiring a flexible cured epoxy encapsulant
  • Potting applications requiring room-temperature cure capability

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear amber
Chemistry Type
Epoxy
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.00 x 10¹³ Ohms⋅cm

Additional Information

Two-Component Epoxy Encapsulant

LOCTITE ABLESTIK 9392

LOCTITE ABLESTIK 9392 is a clear amber, two-component epoxy encapsulant for general potting applications. The system combines a typical mixed viscosity of 17,000 mPa.s (cP) with room-temperature or heat-cure capability and a flexible cured state. Documented substrate classes include metals, wood, many plastics, and rubber.

Two-component epoxy Clear amber Potting encapsulant Flexible cured state Room-temperature or heat cure

Mixed Material

As-Supplied Properties

The available technical data provide mixed-material properties rather than separate component viscosities or densities. These values should therefore be interpreted as applying after the two components are thoroughly combined.

Typical uncured mixed properties
Property Typical value State / context
Technology Epoxy Two-component system
Appearance Clear amber As supplied / mixed system
Mixed viscosity 17,000 mPa.s (cP) Mixed uncured material
Specific gravity 1.0 Mixed uncured material

Preparation, Mixing and Cure

Processing and Cure

Clean and dry all surfaces before application. Thoroughly mix both components until the color is uniform throughout, then apply the fully mixed material to the prepared surfaces or potting area. Where the material is used as an adhesive, gently press the joined surfaces together and maintain contact until cure is complete.

Heat cure16 hours at 82 degC.
Room-temperature cure168 hours at 24 degC.
Low-temperature crystallizationIf crystallization occurs in BIPAX, TRA-PAX, or bulk packaging, a gentle warming cycle of 50 degC for 30 minutes before mixing may be required to redissolve the components.

The cure profiles are guideline recommendations. Actual cure conditions can vary with the application, curing equipment, oven loading, and actual material temperature.

Storage and Handling

The technical data sheet identifies optimal storage at 27 degC or below in the unopened container and a dry location. The supplied U.S. safety data sheet provides a more conservative safety-storage instruction of -40 degC or below. Because these documents differ materially, the publication page should not present a single storage condition as definitive until the applicable current regional storage requirement is confirmed.

Final Cured Material

Cured Properties

The values below are typical laboratory data for the cured material or bonded specimens. Preserve the stated frequency, temperature, and substrate when using these values for product evaluation.

Hardness
60 Shore A

Typical cured physical property.

Volume resistivity
1.00 x 10^13 ohm-cm

Typical cured value at 25 degC.

Tensile strength
6.89 N/mm2

Typical value, equivalent to 1,000 psi.

Typical cured properties and performance
Property Typical result Condition / context
Hardness 60 Shore A Cured material
Dielectric constant 7.0 1 kHz
Dielectric constant 4.3 1 MHz
Volume resistivity 1.00 x 10^13 ohm-cm 25 degC
Lap shear strength 4.14 N/mm2 (600 psi) Glass substrate
Tensile strength 6.89 N/mm2 (1,000 psi) Cured material

Documented Use Scope

Applications

General Potting

Designed for general encapsulation and potting where a two-component epoxy system and flexible cured state are appropriate.

Mixed-Material Assemblies

Documented substrate classes include metals, wood, many plastics, and rubber. Suitability remains dependent on the exact grade, surface condition, preparation, and application design.

Flexible Encapsulation

The cured Shore A hardness of 60 supports evaluation where a flexible epoxy encapsulant is preferred over a rigid cured material.

Technical Support for LOCTITE ABLESTIK 9392

Discuss material conditioning, mixing, potting geometry, cure selection, substrate preparation, and electrical or mechanical evaluation requirements with Krayden. Application trials should confirm the material's behavior in the intended assembly, process, section thickness, and service environment.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers