Loctite Ablestik 8008MD

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8008MD

Main features

  • Thermally conductive
  • Electrically conductive
  • Stencil printing

Product Description

LOCTITE ABLESTIK 8008MD adhesive is designed for medium die attach applications. This thermally and electrically conductive proprietary hybrid product can be applied to a wafer backside by stencil printing and then B-staged in an oven.

LOCTITE ABLESTIK 8008MD can then be cured after die attach in an in-line process. This material has good substrate wetting, controlled bondline thickness was originally known as RP-825-3C1. It is typically used on PPF, Copper and Silver plated CU leadframes.

LOCTITE ABLESTIK 8008MD is designed as a Wafer Back side Coating for die sizes down to 150x150um and should be applied to the wafer and dried before dicing.  The solvent in 8800MD should evaporate before die placement or during slow cure ramp up. Also, Instead of printing the whole wafer, we expect that 8008MD is also suitable for printing smaller dots.

Cure Schedule

  • 30 minute ramp to 175°C + 60 minutes @ 175°C

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
6 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0005 Ohms⋅cm
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
2.6
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
67,500 mPa.s

Leading Brands Trust in Our Products and Services