ABLESTIK 64C

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ABLESTIK 64C

Main features

  • Non-Silver Conductive Bonding
  • Room-Temperature or Heat Cure
  • Seawater-Exposure Assembly Fit

Product Description

LOCTITE ABLESTIK 64C is a two-component, non-silver, electrically conductive epoxy adhesive for assembly bonding. Component A is a dark gray paste and Component B is a clear liquid mixed at 100:5 by weight. The mixed adhesive provides a 40-minute work life at 25 deg C for a 100 g mass and cures for 24 hours at 25 deg C or 1 hour at 70 deg C. Its non-silver conductive formulation is recommended where seawater exposure can corrode silver-based conductive adhesives. The cured material has a typical volume resistivity of 0.02 ohm cm at 25 deg C.

Key features

  • Non-silver conductive formulation: Provides electrically conductive bonding without silver filler for seawater-exposure applications.
  • Room-temperature or heat cure: Cures in 24 hours at 25 deg C or 1 hour at 70 deg C to match the available process.
  • Defined mixed work window: A 40-minute work life at 25 deg C for a 100 g mass supports controlled mixing and assembly.

Applications

Applications include electrically conductive assembly bonding where seawater exposure can corrode silver-based conductive adhesives.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Dark gray paste / Clear liquid
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Resin / Hardener)
Density (g)
3.2 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:5
Thermal Properties
Operating Temperature
-55 to 130 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.44 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.02 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

The 100:5 mix ratio is by weight; component-specific values are listed separately for Part A and Part B.

PropertyValueUnitMethod / condition
Component A appearanceDark gray pasteResin
Component B appearanceClear liquidHardener
Mix ratio, A:B100:5by weightSpecified component ratio
Component A density3.2g/cm^3Typical
Component B density1.0g/cm^3Typical
Work life40minutesMixed material; 100 g mass at 25 deg C
Cure schedule24 at 25 or 1 at 70hours at deg CGuideline room-temperature or heat cure
Component shelf life180days25 deg C; Part A and Part B
Technical properties

After-processing / final-state properties

Final-state values are typical for the cured two-component adhesive under the stated conditions.

PropertyValueUnitMethod / condition
Operating temperature-55 to 130deg CProduct operating range
Coefficient of thermal expansion45ppm/deg CTMA
Thermal conductivity1.44W/(m K)Typical cured material
Volume resistivity0.02ohm cm25 deg C
Tensile lap shear strength5.5N/mm^2Typical cured material