ABLESTIK 568

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK 568

Main features

  • 2.5 x 10^14 ohm-cm Volume Resistivity
  • 2-Hour 95 deg C Cure
  • 3 mil Glass-Fabric-Supported Film

Product Description

LOCTITE® ABLESTIK 568 is a non-conductive epoxy adhesive film designed for substrate-attach applications. The amber film uses a glass-fabric carrier and has a documented thickness of 3 mil. It provides a typical 24-hour work life at 25°C and low-temperature heat-cure options of 2 hours at 95°C or 4 hours at 75°C under continuous pressure. Typical cured properties include thermal conductivity of 0.28 W/(m·K) at 121°C, volume resistivity of 2.5 × 1014 ohm-cm, and dielectric strength of 1,200 V/mil.

Key features

  • Electrically insulating film: Typical cured volume resistivity is 2.5 × 1014 ohm-cm, with dielectric strength of 1,200 V/mil.
  • Low-temperature heat cure: Guideline cure schedules include 2 hours at 95°C or 4 hours at 75°C.
  • Controlled adhesive format: A 3 mil glass-fabric-supported film is available as sheet stock or customer-specific die-cut preforms.

Applications / Suitable for

  • Substrate-attach applications
  • Electrically insulating adhesive-film bonding
  • Assembly processes requiring lower-temperature heat cure
  • Sheet-stock or die-cut adhesive preforms

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber
Chemistry Type
Epoxy Film
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.28 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2.5×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, handling, storage, and guideline cure information for the adhesive film before final processing.

Property Value Unit Method / condition
Technology Epoxy film — Non-conductive adhesive film
Appearance Amber film — TDS appearance; SDS describes the -1-003 construction as translucent
Carrier type Glass fabric — Adhesive-film construction
Adhesive-film thickness 3 mil Documented TDS construction
Specific gravity 1.29 — SDS value for LOCTITE ABLESTIK 568-1-003
VOC content <1 % SDS value for LOCTITE ABLESTIK 568-1-003
Work life 24 hours At 25°C
Shelf life 365 days At -40°C, from date of manufacture
Recommended cure schedule 2 hours At 95°C; guideline recommendation
Alternative cure schedule 4 hours At 75°C; guideline recommendation
Cure pressure 5–10 psi Continuous pressure during the cure cycle
Technical properties

After-processing / final-state properties

Typical thermal, electrical, and bonded-joint properties of the cured adhesive film. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Thermal conductivity 0.28 W/(m·K) At 121°C; test method, orientation, and cure condition not stated
Volume resistivity 2.5 × 1014 ohm-cm Test method, specimen geometry, and cure condition not stated
Dielectric strength 1,200 V/mil Test method, specimen thickness, conditioning, and cure condition not stated
Dielectric constant 4.1 — At 1 kHz
Dissipation factor 0.0076 — At 1 kHz
Lap shear strength — aluminum to aluminum 35.17 (5,100) N/mm² (psi) Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated
Lap shear strength — gold to gold 24.14 (3,500) N/mm² (psi) Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated