ABLESTIK 506

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ABLESTIK 506

Main features

  • Flexible Cured Adhesive
  • 0.9 W/(m K) Thermal Conductivity
  • Reworkable Bonding Material

Product Description

LOCTITE® ABLESTIK 506 is a slightly tacky, flexible epoxy adhesive film designed for bonding materials with severely mismatched coefficients of thermal expansion. The white, glass-fabric-supported film has a documented thickness of 3 mil and is suitable for assembly bonding of plastics, ceramics, and difficult-to-bond metals. Its tack can support component positioning without holding fixtures for approximately 16 hours after removal from frozen storage. Guideline heat-cure schedules include 60 minutes at 150°C, 90 minutes at 125°C, or 3 hours at 100°C.

Key features

  • Flexible adhesive film: Designed for bonding adherends with severely mismatched coefficients of thermal expansion.
  • Thermally conductive and electrically insulating: Typical cured properties include thermal conductivity of 0.9 W/(m·K) at 121°C and volume resistivity of 0.7 × 1013 ohm-cm.
  • Reworkable, tacky construction: Slight tack supports component positioning, while the documented rework procedure uses heating to 125°C followed by mechanical separation.

Applications / Suitable for

  • Assembly bonding of materials with severely mismatched coefficients of thermal expansion
  • Bonding plastics and ceramics
  • Bonding difficult-to-bond metals
  • Applications requiring a flexible, reworkable adhesive film

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White
Chemistry Type
Epoxy Film
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.9 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.7×10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction, handling, storage, and guideline cure information for the adhesive film before final processing.

Property Value Unit Method / condition
Technology Epoxy film — Flexible, slightly tacky adhesive film
Appearance White film — As supplied
Carrier type Glass fabric — Adhesive-film construction
Adhesive-film thickness 3 mil Documented TDS construction
Density / relative density 2.1 — SDS value for LOCTITE ABLESTIK 506-1-003
VOC content <0.1 % SDS value for LOCTITE ABLESTIK 506-1-003
Work life 24 hours At 25°C
Tack duration Approximately 16 hours After removal from frozen storage
Shelf life 183 days At -40°C; TDS property-table value
Recommended cure schedule 60 minutes At 150°C; guideline recommendation
Alternative cure schedules 90 minutes or 3 hours — 90 minutes at 125°C or 3 hours at 100°C; guideline recommendations
Cure pressure 2–10 psi Continuous pressure during the cure cycle
Technical properties

After-processing / final-state properties

Typical thermal, electrical, and bonded-joint properties of the cured adhesive film. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Coefficient of thermal expansion — below Tg 45 ppm/°C Test method and cure condition not stated
Coefficient of thermal expansion — above Tg 350 ppm/°C Test method and cure condition not stated
Thermal conductivity 0.9 W/(m·K) At 121°C; test method, orientation, specimen geometry, and cure condition not stated
Volume resistivity 0.7 × 1013 ohm-cm Test method, specimen geometry, and cure condition not stated
Dielectric strength 1,190 V/mil Test method, specimen thickness, conditioning, and cure condition not stated
Dielectric constant 5.7 — At 1 kHz
Dissipation factor 0.03 — At 1 kHz
Lap shear strength — aluminum to aluminum 1,200 psi Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated
Lap shear strength — gold to gold 750 psi Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers