ABLESTIK 369-3

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

ABLESTIK 369-3

Main features

  • 0.0005 ohm-cm Volume Resistivity
  • 4-Hour 74 deg C Cure
  • Two-Hour Working Window

Product Description

LOCTITE® ABLESTIK 369-3 is a silver-filled, electrically conductive epoxy adhesive for die-attach and general-purpose bonding applications. The polyamine-activated system provides a two-hour work life at 25°C and uses a moderate-temperature guideline cure of 4 hours at 74°C. Typical cured properties include volume resistivity of 0.0005 ohm-cm, Shore D hardness of 80, and aluminum-to-aluminum lap shear strength of 7.6 N/mm² at 25°C.

Key features

  • Electrically conductive: Typical cured volume resistivity is 0.0005 ohm-cm.
  • Moderate-temperature cure: Guideline cure schedule of 4 hours at 74°C.
  • Extended processing window: A two-hour work life at 25°C supports adhesive placement before cure.

Applications / Suitable for

  • Die-attach applications
  • General-purpose conductive bonding
  • Aluminum-to-aluminum bonding under the documented test condition

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Silver
Chemistry Type
Epoxy
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2 hours
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0005 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, work-life, storage, and guideline cure information before final processing.

Property Value Unit Method / condition
Technology Epoxy — Polyamine-activated adhesive system
Appearance Silver paste — Both Part A and Part B
Filler type Silver — Conductive filler
Specific gravity — Part A 3.0 — SDS physical-property value
Specific gravity — Part B 3.4 — SDS physical-property value
Work life 2 hours At 25°C
Guideline cure schedule 4 hours At 74°C
Optimal storage — Part A -40 °C Store at or below -40°C; unopened container
Optimal storage — finished adhesive -40 °C TDS storage recommendation
Technical properties

After-processing / final-state properties

Typical cured-material electrical, physical, and bonded-joint properties. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Hardness 80 Shore D Cure condition and test method not stated
Volume resistivity 0.0005 ohm-cm Test method, specimen geometry, and cure condition not stated
Lap shear strength — aluminum to aluminum 7.6 (1,100) N/mm² (psi) Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated