LOCTITE ABLESTIK 2100A

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2100A

Main features

  • Fast cure
  • High hot/wet adhesion
  • Ultra low moisture absorption

Product Description

LOCTITE ABLESTIK 2100A die attach adhesive is designed for Pb-free array packaging. This product is able to withstand the high reflow temperatures necessary for Pb-free solders @260°C. It is the "Go To" product for conductive laminate.

LOCTITE ABLESTIK 2100A is a low stress, low bleed conductive die attach with ultra low moisture absorption, suitable for laminate packages like BGA and die sizes up to 12.7 x 12.7 mm

Cure Schedule

  • 30 minute ramp to 175°C + 15 minutes @ 175°C

 

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
60 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.05 Ohms⋅cm
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
5.3
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
9,000 mPa.s

Additional Information

ABP 2100A is containing a PFAS anti-bleed agent and will be discontinued as Henkel moves towards greener materials. The direct PFAS-free replacement is ABP 2100ANP, with only minor changes. Notification is planned for January 2026, with the last-time-buy in December 2026.

Loctite Ablestik 2100A is a product that is an almost direct alternative to Loctite Ablestik 2000B.

Loctite Ablestik 2000B is also a conductive die attach for laminates that it is mainly used in Asian regions. For EMEA we have successfully used 2100A as a drop in for use in BGA laminate applications with great success rates.



Ablestik 2100A DSC Curve - Heat flow vs temperature



Notice how the Onset of cure (minimum cure temperature) is about 70°C. Even though we suggest curing at 175°C, as with all products you can adjust the cure schedule (with a lot of trial, error and personal work) according to your final application properties. 

The volume resistivity may be reduced when curing below 175°C (compared to the TDS value), but we expect that some conductivity will be developed.

 