ABchimie 6028UV UV Cure Thixotropic Resin

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

ABchimie 6028UV UV Cure Thixotropic Resin

Main features

  • One-component
  • Fast UV Curing
  • Excellent adhesion to plastics

Product Description

ABChimie® 6028UV is a transparent thixotropic resin coating designed to provide mechanical and environmental protection to electronic components and assemblies. Its thixotropic quality allows for controlled application with high thicknesses (up to 4mm) without sagging. This makes it ideal for encapsulation or localized protection.

ABChimie® 6028UV is acrylic-based and has excellent adhesion to many substrates, including flexible ones like plastics. It cures rapidly under UV light, has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 6028UV is in full compliance with REACH and RoHS regulations.

Product Key Features

  • Transparent, thixotropic UV-curing resin
  • Allows for thick, controlled application without sagging
  • Fast UV cure (mercury lamp) for high-speed processing
  • Solvent-free formulation (no VOCs)

Applications

  • Encapsulation of electronic components requiring high volumes, localized protection, and a thick coating
  • Sensors on PCBs, wire-bonded chips, and reinforcement of solder joints.
  • Can be used to seal plastic casings on PCBs
  • Printed circuit assemblies. 

Product Family

ABCHIMIE 6028UV

1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Thixotropic translucent liquid
Density (g)
1.06 g/cm3
Mechanical Properties
Durometer (Shore D)
45
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1
CTE α1 (alpha 1) is the slope of the Coefficient of thermal expansion in a temperature range below the Glass transition temperature (Tg). It explains how much a material will expand until it reaches Tg.
63 ppm/°C
Coefficient of Thermal Expansion (CTE), α2
CTE α2 (alpha 2) is the slope of the Coefficient of thermal expansion in a temperature range above the Glass transition temperature (Tg). It explains the extent to which a material will expand after it passes Tg.
118 ppm/°C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
100 °C
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-35.5 °C
Physical Properties
Young's modulus
84 MPa

Additional Information

Frequently Asked Questions About ABChimie® 6028 UV

What are typical applications for ABChimie® 6028 UV?


ABChimie® 6028 UV is a UV-curable resin designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:

  • Automotive electronics (e.g., control units, sensors)
  • Industrial automation (e.g., motor drives, PLCs)
  • Consumer electronics (e.g., smart devices, wearables)
  • Other high-reliability electronic assemblies

Why choose ABChimie® 6028 UV?

ABChimie® 6028 UV delivers rapid UV curing, excellent electrical insulation, thixotropic application properties, and strong adhesion to flexible substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.

What is the shelf life of ABChimie® 6028 UV?

ABChimie® 6028 UV has a shelf life of 12 months when stored at 5–30°C in tightly sealed containers. Prior to use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance.

What happens after the shelf life?

Using ABChimie® 6028 UV past its shelf life may alter viscosity, affecting uniformity and application performance. Always use an in-date product for reliable results.

What is the recommended curing method for ABChimie® 6028 UV?

ABChimie® 6028 UV is UV-curable and should be cured with a mercury lamp. The minimum UVA dose is 1000 mJ/cm² for a 1mm thickness. The LED-curable version is ABChimie® 6028 UV LED. Higher UVA doses do not negatively affect final properties.

What is the maximum thickness for ABChimie® 6028 UV?

ABChimie® 6028 UV can be applied up to 4mm due to its thixotropic properties, allowing high-thickness deposits without sagging.

What safety precautions should I take?

Use ABChimie® 6028 UV in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.

Can I adjust the viscosity?

ABChimie® 6028 UV can be customized for variable viscosities. Contact our team for guidance.


Learn More About ABChimie® 6028 UV


ABChimie® 6028 UV is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable resin delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.


Main Advantages of ABChimie 6028 UV

UV Curing

ABChimie® 6028 UV cures rapidly under UV light, enabling integration into both batch and inline production. The resin forms a durable, high-performance layer that protects assemblies while supporting high-throughput manufacturing.

MECHANICAL PROTECTION

ABChimie® 6028 UV cures to a Shore D hardness of 45, providing excellent mechanical protection. This hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.

THIXOTROPIC

ABChimie® 6028 UV is thixotropic: it maintains a stable, non-running consistency at rest but flows easily under shear during application. This ensures precise placement, minimal sagging, and uniform coverage before rapid UV curing.

EXCELLENT ADHESION ON FLEXIBLE SUBSTRATES

ABChimie® 6028 UV bonds strongly to flexible substrates, including plastics and polymer-based PCBs. Its adhesion ensures reliable protection even on surfaces that bend or flex, ideal for wearables, flexible electronics, and lightweight assemblies.


How to Choose a Resin

Selecting the most suitable resin requires consideration of key factors:

  • ✔ Norms & Compliance
  • ✔ Environment / Exposure Conditions
  • ✔ Repairability
  • ✔ Electrical Performance
  • ✔ Application Method
  • ✔ Operating Temperature

Compliance You Can Trust ✅

ABChimie® 6028 UV meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:

  • REACH Compliant
  • RoHS 2011/65/EU Compliant
 

Curing Tip: ABChimie 6028 UV cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.

Ref. Leistung / ref power ln % over wavelength in nm

PTM6000HV-SP thermal impedance versus bondline thickness

Ref. Leistung / ref power ln % over wavelength in nm

Key Curing Properties

Lamp Type
Mercury
Emission Spectrum of Mercury Lamp
200-400 nm
Minimum UVA Dose
1000 mJ/cm2
Coating Thickness
1 mm 

Typical property values shown for reference only and should not be used as specifications.




Alternative to Mercury Lamp Curing of ABChimie 6028 UV

ABChimie 6028 UV is also available in the LED - version, which cures by LED Lamp.

ABChimie 6028 UV LED [Go to 6028 UV LED Product Page↗]

  • Thixotropic resin
  • Fluorescent under UV light
  • Excellent adhesion to flexible substrates
  • Immediate curing with UV LED exposure

Best suited for: High-speed process looking to use LED light for curing

Contact Us → 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers