3M SJ3571

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M SJ3571

Main features

  • Reclosable Loop Fastening
  • Acrylic PSA Installation
  • Configurable Roll Conversion

Product Description

3M Loop Fastener SJ3571 is an adhesive-backed woven nylon loop fastener for reclosable attachments used with a compatible 3M hook fastener. The soft napped loops engage the hook side for repeated opening and closing, while the acrylic pressure-sensitive adhesive mounts the loop to clean prepared surfaces without separate sewing or liquid adhesive. SJ3571 is commonly paired with 3M Hook Fastener SJ3572 and is available in multiple colors, widths, and roll lengths. Its preshrunk construction supports flat installation, and the adhesive is rated for long-term exposure to 93 deg C. The loop side is not a complete fastening system by itself.

Key features

  • Reclosable loop function: Engages a compatible hook fastener for repeated access without screws, snaps, or zippers.
  • Acrylic PSA attachment: Supports manual or automated mounting to clean, prepared surfaces.
  • Configurable roll formats: Color, width, and roll-length options support conversion into application-specific pieces.

Applications

Applications include reclosable attachment of furniture cushions, signs, point-of-purchase displays, panels, and general industrial components.

Product Family

3M SJ3571

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
acrylic
Color
The color
black, white
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
polyolefin with embossed 3M logo
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
3600 μm

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the supplied loop fastener unless another status is shown.

PropertyValueUnitMethod / condition
Available colorsBeige, black, whiteCurrent product options
Loop materialWoven nylonAs supplied
AdhesiveHigh-performance acrylic PSAPressure-sensitive backing
Maximum unmated thickness3.2mmWithout liner; depends on compression
Liner thickness0.1mmPolyolefin liner
Shelf life24monthsOriginal packaging at 16 to 27 deg C and 40 to 60% RH
Technical properties

After-processing / final-state properties

Mated performance requires a compatible hook fastener; peel and cycle values are typical under the stated conditions.

PropertyValueUnitMethod / condition
Engaged thickness3.6mmMated fastener; depends on compression
90 deg peel adhesion2.2lb/in width23 deg C; 304 mm/min; one fastener attached to non-anodized aluminum
Overlap shear strength22lb/in^2Nylon hook to nylon loop; 304 mm/min
Long-term temperature resistance93deg CExposure over days to weeks
Cycle life5,000closuresNylon hook to nylon loop; number of closures before losing 50% of original peel strength

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers