3M SJ3526N

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M SJ3526N

Main features

  • Quick Reclosable Hook Attachment
  • Rubber PSA for Low-Energy Plastics
  • Manual or Automated Installation

Product Description

3M Hook Fastener SJ3526N is the adhesive-backed woven nylon hook side of a reclosable fastening system. Its flexible, self-supporting surface has approximately 300 inverted J-hooks per square inch and engages compatible 3M loop material to close; the strips separate by hand for access. A high-performance rubber pressure-sensitive adhesive attaches the hook backing to clean, prepared substrates, including low-surface-energy plastics. The product is commonly paired with 3M Loop Fastener SJ3527N and is available in multiple colors, widths, and roll lengths. Its pressure-sensitive backing supports manual or automated installation without separate sewing or bulk adhesive bonding.

Key features

  • Quick reclosable fastening: The hook engages compatible loop material to close and separates by hand for repeated access.
  • Rubber PSA attachment: Attaches the hook backing to clean, prepared substrates, including low-surface-energy plastics.
  • Manual or automated installation: The pressure-sensitive backing supports flexible assembly methods without separate sewing or bulk adhesive bonding.

Applications

Applications include indoor reclosable fastening, securing fabric to furniture cushions, point-of-purchase displays and signage, and general industrial attachment with compatible loop material.

Product Family

3M SJ3526N

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
rubber
Color
The color
black, white
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Polytehylene with red printing
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
3600 μm

Additional Information

Technical properties

As-supplied / before-processing properties

SJ3526N is the hook component; a compatible loop fastener is required to form the reclosable system.

PropertyValueUnitMethod / condition
ColorsBlack, whiteStandard listed colors
Hook materialWoven nylonFlexible inverted J-hooks
Adhesive typeRubberPressure-sensitive adhesive
Weight0.062g/cm^2Typical
Maximum unmated thickness2.4mmWithout liner; depends on compression load
LinerPolyethylene with red printingWhite primary liner color
Liner thickness0.08mmTypical
Technical properties

After-processing / final-state properties

Closure values apply to the stated nylon hook-to-loop test configuration and are not adhesive-to-substrate bond values.

PropertyValueUnitMethod / condition
Engaged thickness3.6mmNylon hook to nylon loop; depends on compression load
90 deg peel adhesion3.9g/cm width23 deg C; 304 mm/min; one fastener attached to non-anodized aluminum
Overlap shear strength15.2N/cm^2Nylon hook to nylon loop; 304 mm/min
T-peel adhesion3.5g/cm widthASTM D5170 closure performance; 304 mm/min
Dynamic tensile7.6N/cm^2Nylon hook to nylon loop; 304 mm/min
Cleavage strength13.1g/cm widthNylon hook to nylon loop
Long-term temperature resistance49deg CDays to weeks
Cycle life5,000closuresBefore losing 50% of original peel strength