3M ES-2000

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M ES-2000

Main features

  • Clear High-Gloss Edge Seal
  • Controlled 1:1 Duo-Pak Application
  • 25-Minute Tack-Free Time

Product Description

3M Edge Sealer ES2000 is a two-part clear urethane sealer for protecting exposed film and applique edges. It is supplied in 50 mL dual-syringe Duo-Pak cartridges at a 1:1 mix ratio and contains 100% solids. The sealer cures at ambient conditions to a clear, non-yellowing, high-gloss finish and becomes tack-free in about 25 minutes. Environmental exposure performance is supported by a typical yellowness index of 0.3 initially and 2.3 after 1,000 hours of ASTM G155 Cycle 1 exposure. The cured material reaches a typical Shore C hardness of 64 after 24 hours and 68 after 48 hours.

Key features

  • Clear high-gloss edge seal: Cures at ambient conditions to a transparent, non-yellowing finish for visible film and applique edges.
  • Controlled 1:1 cartridge dispensing: The 50 mL Duo-Pak system proportions both components through the 3M EPX applicator.
  • Environmental exposure performance: A typical yellowness index of 2.3 after 1,000 hours of ASTM G155 Cycle 1 exposure supports long-term appearance assessment.

Applications

Applications include sealing exposed edges of aviation applique and compatible surface-protection films on specified aircraft paints, primers, and films.

Product Family

3M ES-2000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
100 %
Physical Properties
Tack-Free Time
25 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and apply to the two-part ES2000 system.

PropertyValueUnitMethod / condition
ColorClearVisual
Part A viscosity30,000 to 40,000cPASTM D2196; Brookfield RVF No. 3 spindle at 1 rpm and 25 deg C
Part B viscosity1,000 to 5,000cPASTM D2196; Brookfield RVF No. 3 spindle at 10 rpm and 25 deg C
Solids content100%Typical
Mix ratio1:1by volumeDuo-Pak cartridge
Package size50mLDual-syringe Duo-Pak cartridge
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore C hardness64ASTM D2240; after 24 hours
Shore C hardness68ASTM D2240; after 48 hours
Tack-free time25minutesASTM D5895
Yellowness index0.3ASTM E313
Yellowness index after exposure2.3ASTM E313; after 1,000 hours per ASTM G155 Cycle 1

Leading Brands Trust in Our Products and Services