3M EC-9300

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-9300

Main features

  • Five-Hour Assembly Work Life
  • Room-Temperature or Mild-Heat Cure
  • Qualified Aircraft Interior FST Data

Product Description

3M Scotch-Weld Epoxy Adhesive EC-9300 B/A FST is a two-part, room-temperature-curing structural epoxy adhesive for aircraft interior assembly. Part B and Part A mix at 100:50 by volume and provide a five-hour work life at 23 +/- 2 deg C for a 45 g mixed quantity. The non-sag adhesive reaches full cure in seven days at 23 deg C or two hours at 65 deg C. Standalone and aluminum-backed specimens were tested for flammability under FAR/JAR/CS 25.853. Separate standalone specimens were evaluated for smoke density under FAR/JAR/CS 25.853 and AITM 2.0007 and for toxic-gas emission under Airbus ABD0031 and AITM 3.0005. The values apply only to those tested configurations.

Key features

  • Five-hour assembly window: Provides a defined work life at 23 +/- 2 deg C for the stated 45 g mixed quantity.
  • Room-temperature or mild-heat cure: Reaches full cure in seven days at 23 deg C or two hours at 65 deg C.
  • Qualified aircraft interior FST scope: Flammability data covers standalone and aluminum-backed specimens; smoke-density and toxic-gas data covers the stated standalone specimens.

Applications

Applications include aircraft interior structural bonding, metal-to-honeycomb and honeycomb-panel bonding, insert bonding, and ditch-and-pot assembly.

Product Family

3M EC-9300

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Part B and Part A values are shown in the source order; technical values are typical.

PropertyValueUnitMethod / condition
Part B colorBrownAs supplied
Part A colorOff-whiteAs supplied
Part B density1.22g/cm^3Typical
Part A density1.17g/cm^3Typical
Part B viscosity190Pa sTypical
Part A viscosity15Pa sTypical
Mix ratio, Part B:Part A100:50by volumeSpecified product ratio
Work life5hours45 g mixed adhesive at 23 +/- 2 deg C
Technical properties

After-processing / final-state properties

Values are typical for clad aluminum 2024-T3 prepared by optimized FPL. Unless stated otherwise, specimens were cured 2 hours at 65 deg C and used about 1 wt% glass beads, 90 to 150 um diameter, to control bondline thickness.

PropertyValueUnitMethod / condition
Overlap shear strength24MPaEN 2243-1; -55 deg C test
Overlap shear strength29MPaEN 2243-1; 23 deg C test
Overlap shear strength11MPaEN 2243-1; 80 deg C test
Overlap shear strength, room-temperature cure27MPaEN 2243-1; 7 days at 23 deg C; tested at 23 deg C
Floating roller peel strength102N/25 mmEN 2243-2; tested at 23 deg C
Overlap shear strength after hot-wet aging21MPaEN 2243-1; 168 h at 100% RH and 55 deg C; tested at 23 +/- 2 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers