3M EC-3924

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3924

Main features

  • Bondline Corrosion Protection
  • Spray Brush or Roller Application
  • Controlled Film and Bake Process

Product Description

3M Scotch-Weld Structural Adhesives Primer EC-3924B is a single-component, corrosion-inhibiting epoxy primer for prepared metal surfaces used with compatible 250 deg F-curing 3M structural adhesive films. It protects cleaned metal inside and outside the bondline and can also serve as a corrosion-resistant coating. The primer can be sprayed, brushed, or rolled after warming to ambient temperature and thoroughly agitating to redisperse settled pigment. Recommended dry-film thickness is 0.05 to 0.15 mil inside the bondline and 0.05 to 0.3 mil outside it. The recommended bake cycle is 30 minutes at 24 deg C followed by 60 minutes at 121 +/- 5.6 deg C.

Key features

  • Bondline corrosion protection: Protects cleaned metal surfaces inside and outside the adhesive bondline.
  • Spray, brush, or roller application: Supports three practical coating methods for prepared metal components.
  • Controlled film and bake process: Defined dry-film ranges and a two-stage bake cycle support consistent primer application before bonding.

Applications

Applications include priming prepared metal before bonding with compatible 250 deg F-curing 3M structural adhesive films and protecting metal surfaces inside and outside the bondline.

Product Family

3M EC-3924

Loading pricing…

Technical Specifications

General Properties
Color
The color
Yellow
Solids
6 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-14.4 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceYellow thin liquidAs supplied
Net weight7.4 +/- 0.2 (0.887 +/- 0.024)lb/gal (kg/L)Typical
Solids content6 +/- 1.0%Typical
Flash point6 (-14.4)deg F (deg C)TEC
Storage temperature0 or below (-18 or below)deg F (deg C)Original unopened container
Shelf life6monthsFrom shipment; stored at 0 deg F (-18 deg C) or below

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers