3M EC-3542

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3542

Main features

  • Flame Retardant Interior Assembly
  • Low Density Insert Bonding
  • Controlled Non Sag Work Life

Product Description

3M Scotch-Weld Epoxy Adhesive EC-3542 B/A FR is a light-gray, low-density, flame-retardant two-part epoxy for structural bonding of prepared metals and composites and for insert bonding in aircraft-interior assemblies. The 100% solids, thixotropic mixture uses a 100:50 volume ratio and provides approximately 30 minutes of work life at 22 deg C. Its non-sag consistency controls placement around inserts and vertical bondlines. After cure, the adhesive reaches 50 MPa compressive strength at 24 deg C and 2036 psi aluminum overlap shear with the specified room-temperature and heat-cure schedule.

Key features

  • Flame Retardant Interior Bonding: The cured material meets the cited 14 CFR 25.853(a) specimen test before and after conditioning.
  • Low Density Insert Placement: A cured density of 0.71 g/cm3 supports lightweight bonded insert assemblies.
  • Thirty Minute Non Sag Work Life: Thixotropic flow provides positioning time without uncontrolled migration.

Applications

Prepared metal and composite structural bonding, insert bonding, and aerospace-interior assembly within the qualified flame-test configuration.

Technical Specifications

General Properties
Density (g)
0.71 g/cm3
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
30 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorWhite-Epoxy component
Part A colorGray-Amine component
Mix ratio by weight100:52B:ATwo-part system
Mix ratio by volume100:50B:ATwo-part system
Solids100%Both components
Work lifeApproximately 30minAt 22 deg C
ConsistencyThixotropic-Mixed adhesive
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorLight gray-Cured
Density0.71g/cm3Cured; typical
Volatile lossLess than 0.1%During cure
Compressive strength50MPaTested at 24 deg C
Compression modulus1427MPaTested at 24 deg C
Overlap shear strength2036psiPrepared aluminum; specified room-temperature and heat cure
Insert pull strength1792NTested insert configuration
Insert torque12.3N-mTested insert configuration