3M EC-3532

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3532

Main features

  • Tough Impact Resistant Assembly
  • Rapid Non Sag Placement
  • Primed Multi Material Bonding

Product Description

3M Scotch-Weld Urethane Adhesive EC-3532 B/A is a two-part polyurethane adhesive that cures at room temperature or with heat to form tough, impact-resistant bonds. It adheres to many primed or painted metals and selected plastics, while the mixed material becomes non-sag in approximately 30 seconds for controlled placement on vertical or irregular joints. Equal-volume mixing and a 5 to 15 minute work life at 24 deg C support practical alignment before fixturing. After cure, prepared aluminum overlap shear reaches 2200 psi at 24 deg C and 2500 psi at -40 deg C.

Key features

  • Tough Impact Resistant Bonding: The cured polyurethane supports assemblies exposed to shock and service movement.
  • Rapid Non Sag Control: The mixed adhesive resists sagging in approximately 30 seconds.
  • Primed Metal And Plastic Adhesion: The urethane bonds many compatible primed or painted substrates.

Applications

Bonding primed or painted metals, selected plastics, and industrial or aerospace assemblies requiring tough, impact-resistant joints.

Product Family

3M EC-3532

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Brown
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100 :100
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5-15 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorOff white-Polyol component
Part A colorBrown-Isocyanate component
Mix ratio by weight100:109B:ATwo-part system
Mix ratio by volume100:100B:ATwo-part system
Base viscosity10000 to 55000cPAt 24 deg C
Accelerator viscosity15000 to 40000cPAt 24 deg C
Work life5 to 15min100 g mixed at 24 deg C
Non-sag developmentApproximately 30secAfter mixing
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorBrown-Cured
Full cure24hAt 24 deg C
Overlap shear strength2500psiEtched aluminum; tested at -40 deg C
Overlap shear strength2200psiEtched aluminum; tested at 24 deg C
Overlap shear strength300psiEtched aluminum; tested at 82 deg C
Overlap shear strength700psiPolycarbonate; tested at 24 deg C