3M EC-3515

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3515

Main features

  • Lightweight Aerospace Void Filling
  • Honeycomb Edge Sealing Control
  • Flexible Ambient Or Heat Cure

Product Description

3M Scotch-Weld Void Filling Compound EC-3515 B/A FR is a two-part, low-density, flame-retardant epoxy compound for void filling, honeycomb-edge sealing, and abradable filling in aerospace interior structures. The 1:1 volume ratio produces a blue or black dough-like mixture with more than 90 minutes of work life for a 200 g batch. Processing can remain at room temperature, with cure completed in two days at 23 deg C or accelerated to five hours at 52 deg C. After cure, the material reaches Shore D 57 hardness and 21 MPa compressive strength at 24 deg C.

Key features

  • Low Density Void Filling: A mixed density of 0.47 to 0.50 g/cm3 supports lightweight cavity filling.
  • Edge Sealing And Finishing: The dough-like compound can fill honeycomb edges and abradable areas.
  • Ambient Or Accelerated Cure: The epoxy cures in two days at 23 deg C or five hours at 52 deg C.

Applications

Aerospace honeycomb-edge sealing, structural void filling, abradable filling, and aircraft-interior repair within the qualified process.

Product Family

3M EC-3515

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.50 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorBlue or black-Epoxy component
Part A colorWhite-Modified amine component
Mix ratio by weight100:94B:ATwo-part system
Mix ratio by volume1:1B:ATwo-part system
Solids100%Mixed compound
Mixed density0.47 to 0.50g/cm3Before cure
Work lifeMore than 90min200 g mixed batch
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorBlue or black-Cured
Hardness57Shore DCured
Compressive strength37MPaTested at -55 deg C
Compressive strength21MPaTested at 24 deg C
Compressive strength3.1MPaTested at 93 deg C
Compression modulus825MPaTested at 24 deg C
Room-temperature cure2daysAt 23 deg C
Accelerated cure5hAt 52 deg C