3M EC-3500

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3500

Main features

  • Low Density Core Splicing
  • Edge And Void Filling
  • Multi Step Panel Assembly

Product Description

3M Scotch-Weld Core Splice Adhesive EC-3500 B/A is a two-part, low-density epoxy compound developed for honeycomb-core splicing, panel-edge filling, and localized void filling in aerospace sandwich structures. Its paste format allows material to be placed at core joints and irregular cavities before panel closeout. The same system can address adjacent honeycomb sections, exposed core edges, and local gaps without changing material types between these panel-building steps. It is intended for controlled Part A and Part B preparation within the exact EC-3500 process selected for the assembly.

Key features

  • Honeycomb Core Splicing: The low-density epoxy joins adjacent core sections in sandwich-panel construction.
  • Edge And Void Filling: The compound fills exposed panel edges and localized cavities around core details.
  • Two Part Process Control: Separate Part A and Part B components are prepared for the intended assembly step.

Applications

Honeycomb-core splicing, aerospace sandwich-panel assembly, exposed-edge filling, and localized void filling.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two
Physical Properties
Volatiles
Less than 1 %