3M EC-3439

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3439

Main features

  • Low Density Core Reinforcement
  • Extended One Part Shop Life
  • High Temperature Cured Performance

Product Description

3M Scotch-Weld Structural Adhesive EC-3439 HT is a beige, one-part modified epoxy void-filling compound for honeycomb-core reinforcement, edge finishing, insert bonding, and aircraft sandwich-panel work. Its cured density is below 0.75 g/cm3, and press-flow time is about 90 seconds at 26 deg C using the specified 4 bar, 2.6 mm orifice test. The material provides up to four days of shop life at 15 to 25 deg C and heat cures for one hour at 125 to 175 deg C. Cured compression and overlap-shear values cover subzero, room, and elevated test temperatures.

Key features

  • Low Density Void Filling: The cured compound remains below 0.75 g/cm3 for lightweight core detailing.
  • Four Day Shop Life: The one-part material can remain at 15 to 25 deg C for up to four days before processing.
  • High Temperature Heat Cure: A one-hour cure window from 125 to 175 deg C supports controlled aerospace processing.

Applications

Honeycomb-core reinforcement, panel-edge finishing, insert bonding, local void filling, and aerospace sandwich-panel assembly.

Technical Specifications

General Properties
Color
The color
Beige

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ChemistryModified epoxy-One-part compound
ColorBeige-As supplied
Press-flow timeApproximately 90sec20 g at 26 deg C; 4 bar; 2.6 mm orifice
Shop lifeUp to 4daysStored at 15 to 25 deg C before processing
Heat-cure time1hAt 125 to 175 deg C; heat-up rate 2 to 5 deg C/min
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Cured densityLess than 0.75g/cm3After cure
Compressive strength52.5MPaTested at 23 deg C after 125 deg C cure
Compressive strength65.4MPaTested at 23 deg C after 175 deg C cure
Compressive strength27.1MPaTested at 175 deg C after 125 deg C cure
Compressive strength38.1MPaTested at 175 deg C after 175 deg C cure
Overlap shear strength9.3MPaTested at -55 deg C after 175 deg C cure
Overlap shear strength8.8MPaTested at 23 deg C after 175 deg C cure
Overlap shear strength9.4MPaTested at 175 deg C after 175 deg C cure