3M EC-2615

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-2615

Main features

  • Tough Impact Resistant Bonding
  • High Shear And Peel Performance
  • Non Sag Assembly Control

Product Description

3M Scotch-Weld Epoxy Adhesive EC-2615 B/A is a 100% solids, two-part non-sag epoxy for tough, impact-resistant bonds on prepared metal and selected plastic substrates. Mix Part B and Part A at 100:50 by volume; the off-white base and amber accelerator provide more than 20 minutes of work life for a 20 g batch at 22 deg C. After a seven-day room-temperature cure, prepared aluminum bonds reach 5500 psi overlap shear, 73 piw T-peel strength, and 98 piw floating-roller peel strength under the stated test conditions.

Key features

  • Tough Impact Resistant Bond: The cured epoxy supports structural joints exposed to impact and service stress.
  • High Shear And Peel Strength: Prepared metal assemblies benefit from strong shear and peel performance.
  • Non Sag Application Control: Thixotropic consistency helps retain adhesive on vertical or irregular joints.

Applications

Structural bonding of prepared metal and selected plastic parts, including assemblies that need non-sag placement and impact resistance.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Accelerator| Base)
Other Properties
Storage Temperature
15- 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorOff white-Before mixing
Part A colorAmber-Before mixing
Mix ratio by weight100:49B:ATwo-part system
Mix ratio by volume100:50B:ATwo-part system
Solids100%Both components
Work lifeMore than 20min20 g mixed at 22 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Overlap shear strength5500psiAluminum; 7 day room-temperature cure; tested at 24 deg C
Conditioned overlap shear strength4400psiAluminum; 14 days at 71 deg C and 100% RH; tested at 24 deg C
T-peel strength73piwAluminum; ASTM D1876 at 24 deg C
Floating roller peel strength98piwAluminum; ASTM D3167 at 24 deg C