3M DP605NS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M DP605NS

Main features

  • Tough Flexible Urethane Bond
  • Five Minute Assembly Work Life
  • Non Sag Placement Control

Product Description

3M Scotch-Weld Urethane Adhesive DP605NS, Off-White is a two-part, non-sag urethane adhesive that forms tough, flexible bonds on prepared wood, selected plastics, painted metals, ceramics, and glass. The 1:1 mix ratio and 5 minute work life support fast assembly, while the thixotropic consistency controls placement on vertical or contoured joints. Handling strength develops in 15 to 20 minutes at 23 deg C. The cured off-white adhesive combines 100% elongation with peel and overlap-shear performance for assemblies that require flexibility.

Key features

  • Tough Flexible Urethane Bond: The cured adhesive combines structural attachment with 100% elongation.
  • Five Minute Assembly Work Life: The fast work life supports rapid placement and fixturing.
  • Non Sag Placement Control: Thixotropic consistency resists running on vertical and contoured joints.

Applications

Bonding prepared wood, selected plastics, painted metals, ceramics, glass, and flexible industrial assemblies.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-White
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two
Other Properties
Storage Temperature
15 - 27 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.0 x 10¹⁴ Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
41 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorWhite-Before mixing
Part A colorTan-Before mixing
Mix ratio by volume1:1B:ATwo-part system
Mix ratio by weight1:1B:ATwo-part system
Part B density8.8 to 9.2lb/galAs supplied
Part A density9.7 to 10.2lb/galAs supplied
Work life5min10 g mass, 1/4 in thick at 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorOff white-Cured
Hardness60 to 65Shore DASTM D2240
Elongation100%ASTM D882 basis
Glass transition temperature41deg CDSC, second heat
Overlap shear on aluminum650psiASTM D1002 at 23 deg C; MEK, abrade, MEK preparation
Floating roller peel on aluminum33piwASTM D3167 at 23 deg C