3M DP604NS

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M DP604NS

Main features

  • 4-Minute Open Time
  • 1:1 Meter-Mix Processing
  • 51 to 121 deg C Service Range

Product Description

3M™ Scotch-Weld™ Urethane Adhesive DP604NS Black is a rapid-setting, two-component polyurethane adhesive supplied in a 1:1 ratio duo-pak cartridge. The EPX™ dispensing system mixes the components into a bubble-free, non-sag black paste for structural bonding and sealing. The mixed adhesive provides a 4-minute open time and reaches set strength in approximately 20 minutes at 23 °C. After cure, it combines 85 Shore A hardness with 420% strain at break and a continuous temperature range of -51 to 121 °C. Applications include manufacturing and assembly, building maintenance and repair, bonding door frames and sills, and general structural bonding and sealing.

Key features

  • Rapid-setting formulation: Provides a 4-minute open time and approximately 20-minute set time at 23 °C.
  • Controlled 1:1 dispensing: Duo-pak packaging supports automatic component mixing and bubble-free application through the 3M™ EPX™ system.
  • Flexible cured performance: Delivers 420% strain at break, 85 Shore A hardness, and a continuous temperature range of -51 to 121 °C.

Applications / Suitable for

  • Manufacturing and assembly
  • Building and construction maintenance and repair
  • Bonding wood or metal door sills to concrete
  • Bonding wood and metal door frames to supporting structures
  • General structural bonding and sealing

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black
Density (g)
B: 8.3 — 8.7/A: 8.5 — 8.9 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Solids
100 %
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
4 mins hours
Physical Properties
Open time
4 minutes
Viscosity (Part A)
1500 — 3500 mPa.s
Viscosity (Part B)
800 — 2000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
420 %
Peel Strength
58 N/cm
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
(-51)- 121 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the individual components and mixed adhesive. These values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
Mixed color Black — Typical mixed adhesive
Mix ratio by volume 1:1 B:A As supplied in a duo-pak cartridge
Base viscosity 800–2,000 cP 23 °C; Brookfield CP #3 at 20 rpm
Accelerator viscosity 1,500–3,500 cP 23 °C; Brookfield CP #3 at 20 rpm
Open time 4 min Maximum time after application before the bond is closed and fixed
Work life 4 min 10 g mixed adhesive at 23 °C
Set time 20 min 23 °C; minimum time to reach 0.3 MPa overlap shear strength
Technical properties

After-processing / final-state properties

Typical cured and bonded performance values under the stated test conditions. Results may vary with substrate, preparation, bondline, and curing conditions.

Property Value Unit Method / condition
Cured color Black — Typical cured adhesive
Modulus 6,700 lb/in² ASTM D638 / ISO 527 at 23 °C
Strain at break 420 % ASTM D638 / ISO 527 at 23 °C
Shore A hardness 85 Shore A ASTM D2240 at 23 °C
Continuous temperature range -51 to 121 °C Typical cured characteristic
Overlap shear strength — aluminum 650 lb/in² ASTM D1002 / ISO 4587; 23 °C; 7-day dwell; MEK/abrade/MEK preparation
Overlap shear strength — polycarbonate 720 lb/in² ASTM D1002 / ISO 4587; 23 °C; 7-day dwell; IPA wipe/abrade/IPA wipe
Bell peel 33 lb/in width ASTM D3167; etched aluminum; 23 °C