Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M DP460NS

Main features

  • Non-Sag Placement Control
  • 60-Minute Working Window
  • High Shear and Peel Strength

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive DP460NS is an off-white, non-sag, toughened, two-part structural epoxy adhesive formulated for durable bonding across metals, ceramics, glass, wood, composites and selected plastics. It combines a 2:1 mix ratio by volume with a 60-minute work life, allowing time for adhesive application, joint assembly and repositioning. DP460NS develops handling strength in approximately four hours and reaches full cure in 24 hours at 23°C.

Key features

  • Non-sag formulation: Supports controlled adhesive placement on vertical surfaces and assemblies where flow must be limited.
  • 60-minute work life: Provides an extended assembly window for positioning and adjustment before cure progresses.
  • High shear and peel strength: Provides durable structural bonding with documented overlap shear and T-peel performance.
  • Toughened epoxy performance: Supports bonded assemblies exposed to impact, vibration and demanding service conditions.
  • Cartridge or bulk supply: Compatible with 3M™ EPX™ dispensing equipment and two-part production dispensing systems.

Suitable for

  • Structural bonding of metals and prepared composite materials
  • Assemblies requiring extended positioning time and non-sag application
  • Bonding ceramics, glass, wood and selected engineering plastics

Relevant resources

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-White
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
B/A: 2/1
Solids
100 %
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
1 hours
Physical Properties
Viscosity (Part B)
150,000 — 275,000 mPa.s
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
3.25 x 10¹⁵ Ohms⋅cm

Additional Information

Non-sag structural epoxy adhesive

3M™ Scotch-Weld™ Epoxy Adhesive DP460NS

3M™ Scotch-Weld™ DP460NS is an off-white, non-sag, toughened, two-part epoxy adhesive for demanding structural bonding. Its 60-minute work life provides time for application, positioning and assembly, while the cured adhesive delivers documented shear, peel, electrical and environmental performance across supported substrates.

Two-part epoxy Non-sag 2:1 mix ratio 60-minute work life Toughened
3M Scotch-Weld Epoxy Adhesive DP460NS off-white Duo-Pak cartridge and product packaging

Non-sag, toughened structural epoxy available in Duo-Pak cartridges and bulk containers.

As supplied and mixed

Key processing properties

DP460NS combines high-viscosity, non-sag rheology with an extended working window. The epoxy base and amine accelerator must be accurately proportioned and thoroughly mixed before application.

Mix ratio by volume
2:1
Part B epoxy base to Part A accelerator.
Work life
60 min
Typical at 23°C for documented mixed quantities.
Handling strength
Approx. 4 h
Typical at 23°C.
Full cure
24 h
Published room-temperature cure at 23°C.
Typical uncured and mixed properties
Property Typical value Condition and test method
Base resin (Part B) Epoxy -
Accelerator resin (Part A) Amine -
Base viscosity 150,000–275,000 mPa·s Approximate at 23°C
Accelerator viscosity 8,000–14,000 mPa·s Approximate at 23°C
Mix ratio by weight, B:A 2:0.96 -
Color after cure Off-white Cured adhesive

Technical values are representative or typical and must not be interpreted as guaranteed product specifications.

Processing

Surface preparation, dispensing and cure

DP460NS may be dispensed from Duo-Pak cartridges using compatible 3M™ EPX™ equipment or proportioned through two-part bulk dispensing systems. Surface condition, proportioning, mixing and joint control materially affect bonded-joint performance.

Prepare the substrates: Remove oils, dust, loose oxides, paint, mold-release agents and other contamination. Select preparation according to substrate and required bond durability.
Meter and mix: Dispense at 2:1 by volume. For manual or bulk mixing, use the documented 2:0.96 ratio by weight and mix completely until uniform.
Apply and assemble: Apply to clean, dry surfaces and complete positioning within the available working time. The non-sag formulation helps limit flow after placement.
Secure and cure: Hold the joint in position until handling strength develops. Full room-temperature cure is published as 24 hours at 23°C; heat may accelerate strength development when appropriate for the assembly.
Surface preparation, 2 to 1 dispensing, static mixing, non-sag adhesive application and curing process for 3M Scotch-Weld DP460NS

Recommended visual: cleaning and abrasion, 2:1 dispensing, static mixing, adhesive placement, joint assembly and cure.

Storage and handling

Keep both components in their original packaging and protect them from contamination, excessive heat and direct sunlight. Follow the storage limits and shelf-life information printed on the product packaging and current manufacturer documentation. Review the applicable safety documentation before handling either component.

Bonded-joint performance

Shear and peel performance

DP460NS provides documented overlap shear and peel performance across multiple temperatures. Every result remains specific to the stated substrate, surface preparation, cure, bondline geometry and test method.

Aluminum overlap shear
32.1 MPa
Typical at 23°C on etched aluminum after the documented cure.
T-peel at 23°C
105 N/cm
60 lb/in width on aluminum using ASTM D1876.
T-peel at 82°C
35 N/cm
20 lb/in width on aluminum using ASTM D1876.
Typical aluminum overlap shear by test temperature
Test temperature Typical value Context
−55°C 33.8 MPa Etched aluminum; overlap shear
23°C 32.1 MPa Etched aluminum; overlap shear
82°C after 15 min 9.4 MPa Time in test chamber before testing
82°C after 4 h 18.5 MPa Time in test chamber before testing
121°C after 15 min 2.9 MPa Time in test chamber before testing

The reported strength values are laboratory test results and are not universal design allowables. Confirm performance in the intended substrate system, joint geometry and operating environment.

Bonded-joint performance

Substrate-specific overlap shear strength

The following typical values were measured at 23°C after seven days using ASTM D1002 or ISO 4587. Results remain specific to the listed substrate, preparation, specimen dimensions, bondline and test rate.

Typical overlap shear strength at 23°C after seven days
Substrate Surface preparation Value (Psi) Value (Mpa)
Aluminum MEK / abrade / MEK 2,670 psi 18.4 Mpa
Cold rolled steel MEK / abrade / MEK 3,600 psi 24.8 Mpa
Stainless steel MEK / abrade / MEK 2,400 psi 16.5 Mpa
Copper MEK / abrade / MEK 4,400 psi 30.3 Mpa
Brass MEK / abrade / MEK 3,400 psi 23.5 Mpa
ABS IPA wipe / abrade / IPA wipe 572 psi 4.0 Mpa
Polycarbonate IPA wipe / abrade / IPA wipe 390 psi 2.7 Mpa
Acrylic IPA wipe / abrade / IPA wipe 270 psi 1.9 Mpa
Fiber-reinforced plastic IPA wipe / abrade / IPA wipe 1,379 psi 9.5 Mpa
PVC IPA wipe / abrade / IPA wipe 313 psi 2.15 Mpa

Specimens used a 25 mm width, 12.7 mm overlap and 0.13–0.20 mm bondline. Separation rate was 2.5 mm/min for metals and 51 mm/min for plastics.

Peel performance

Bell peel and T-peel adhesion

Peel data should be evaluated separately from overlap shear because specimen geometry, peel angle, adherend flexibility and test rate differ.

Bell peel on aluminum, ASTM D3167
Temperature Typical value
−55°C 19 lb/in width
23°C 77 lb/in width
82°C 39 lb/in width
T-peel on aluminum, ASTM D1876
Temperature Typical value
−55°C 3–5 lb/in width
23°C 60 lb/in width
82°C 20 lb/in width

Bell-peel testing used 12.7 mm wide bonds, 1.6 mm bondlines and 15 cm/min jaw separation. T-peel testing used 25 mm wide bonds and 508 mm/min jaw separation.

Cured adhesive

Physical properties

The following values characterize the cured bulk adhesive. They do not independently establish performance of a complete bonded assembly.

Typical cured-material properties
Property Test method or condition Typical value
Cured color Visual Off-white
Shore D hardness ASTM D2240 at 23°C 81
Flammability classification Industry specification UL 94 HB
Cured adhesive

Thermal and electrical properties

The cured adhesive provides documented hardness, thermal-expansion and electrical-resistivity properties. These bulk-material results should not be treated as proof of complete assembled-joint performance.

Shore D hardness
78–84
Typical cured-material range.
CTE below Tg
74.44 × 10−6
m/m/°C.
CTE above Tg
166 × 10−6
m/m/°C.
Volume resistivity
3.25 × 1015 Ω·cm
ASTM D257 at 23°C.
Applications

Structural bonding applications

DP460NS is suitable for industrial structural bonding where extended work life, non-sag placement and durable shear and peel performance are important selection factors.

Metal structural assemblies

Documented adhesion data support evaluation on prepared aluminum, steel, copper, brass and stainless-steel substrates.

Composite and engineered-material bonding

The toughened formulation may be evaluated for bonding fiber-reinforced plastics and other supported composite materials after suitable preparation.

Complex or vertical assemblies

Non-sag rheology and a 60-minute work life support controlled placement and extended positioning on larger or more complex assemblies.

Product resources

Structural adhesive guidance

Use these 3M technical resources to support surface preparation, dispensing-system setup, structural adhesive selection and understanding of toughened adhesive performance.

Surface Preparation and Pretreatment

Technical guidance covering cleaning, abrasion and pretreatment considerations for structural adhesive bonding.

View technical bulletin

Structural Adhesive Dispensing Instructions

Instructions and troubleshooting information for cartridge dispensing and static mixing of two-part structural adhesives.

View dispensing guide

3M’s Tough Stuff

A white paper discussing toughened structural adhesive technology and the role of adhesive toughness in durable bonded joints.

Read the white paper

Choosing and Using a Structural Adhesive

Selection guidance covering substrates, joint design, processing requirements and performance considerations for structural adhesives.

Read selection guidance
Next steps

Evaluate 3M™ Scotch-Weld™ DP460NS for your structural assembly

Contact Krayden to review substrate preparation, dispensing equipment, working-time requirements, bondline design, cure conditions and application-specific mechanical or environmental testing for your structural bonding process.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers