3M DP460EG

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M DP460EG

Main features

  • Long Work Life Assembly
  • Low Outgassing Electronics Bonding
  • Toughened Structural Epoxy

Product Description

3M Scotch-Weld Epoxy Adhesive DP460EG is a toughened, two-part electronics-grade epoxy with a 2:1 mix ratio and a 110 minute work life. The long processing window supports precise bonding, fixing, rigidizing, potting, and magnet assembly before handling strength develops in approximately four hours. DP460EG combines strong structural bonding with controlled total and siloxane outgassing for sensitive assemblies. Room-temperature cure is available, while elevated-temperature schedules accelerate cure and can increase glass-transition performance in controlled production environments.

Key features

  • Long Work Life Assembly: The 110 minute work life supports precise placement and multi-step assembly.
  • Low Outgassing Electronics Bonding: Controlled total and siloxane outgassing supports sensitive electronic components.
  • Toughened Structural Epoxy: The cured adhesive provides high overlap shear and peel performance on prepared aluminum.

Applications

Hard disk drive assembly, bearing and spindle components, magnet bonding, fixing, rigidizing, and potting.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Base / Accelerator)
Other Properties
Storage Temperature
15 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Mix ratio by volume2:1B:ATwo-part system
Mix ratio by weight2.0:0.96B:ATwo-part system
Base colorWhite-Before mixing
Accelerator colorAmber-Before mixing
Base viscosity25 to 45Pa.sAt 23 deg C
Accelerator viscosity8 to 14Pa.sAt 23 deg C
Mixed viscosity15 to 25Pa.sAt 23 deg C
Work life110minAt 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Total outgassingLess than 1000ug/gGC/MS; 85 deg C for 3 h; ASTM 5116 basis
Siloxane outgassing5 maximumug/gGC/MS; 85 deg C for 3 h; ASTM 5116 basis
Thermal conductivity0.263W/mKAt 45 deg C
Dielectric constant4.6-1 kHz at 23 deg C
Dielectric strength35.8V/mil31 mil specimen
Overlap shear strengthGreater than 35.5MPaEtched aluminum; 24 h cure at 23 deg C
T-peel strength10.55N/mmAnodized aluminum; 24 h cure at 23 deg C