3M DP105

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M DP105

Main features

  • Retains Its Clear
  • Flexible Cured Adhesive
  • 4-Minute Working Window

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast-setting, very flexible, two-part epoxy adhesive. Engineered with a 1:1 mix ratio, this versatile formulation is ideal for bonding dissimilar surfaces where differing thermal coefficients of expansion may pose challenges. It uniquely retains its clear, colorless properties longer than most standard 5-minute epoxies, making it suitable for applications requiring both high peel strength and a clean appearance.

Key features

  • Highly flexible: Retains elasticity when cured, making it ideal for bonding dissimilar materials subject to thermal expansion.
  • Clear appearance: Formulated to remain clear and colorless significantly longer than typical 5-minute epoxies.
  • Fast-setting strength: Provides a 4-5 minute work life with rapid strength buildup and high peel performance.

Applications / Suitable for

  • Bonding dissimilar surfaces subject to thermal expansion
  • Applications requiring a clear, colorless adhesive line
  • Assemblies requiring high peel strength and flexibility

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Chemistry Type
B: Epoxy/ A: Mercaptan
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Solids
100 %
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
5 minutes hours
Physical Properties
Net Weight
A: 11.3- 11.7/B:10.9-11.7 kg/m3
Open time
5 minutes
Tack-Free Time
10 minutes
Viscosity (Part A)
8,000-16,000 mPa.s
Viscosity (Part B)
1,000-5,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
120 %
Peel Strength
61 N/cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
8 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.15 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.5 x 10¹⁰ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 1:1 - B:A
Mix Ratio by Weight 1:0.97 - B:A
Color Clear - Base
Color Clear - Accelerator
Base Resin Epoxy - -
Accelerator Resin Mercaptan - -
Base Net Weight 1.09-1.14 g/cm³ (9.1-9.5 lb/gal)
Accelerator Net Weight 1.13-1.17 g/cm³ (9.4-9.8 lb/gal)
Viscosity 1,000-5,000 cP Base at 27°C (80°F)
Viscosity 8,000-16,000 cP Accelerator at 27°C (80°F)
Open Time 5 minutes -
Tack Free Time 10 minutes 3M C3173
Set Time 20 minutes at 23°C (73°F)
Worklife 5 minutes 2g mixed at 23°C (73°F)
Worklife 4 minutes 20g mixed at 23°C (73°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Cured Color Clear - -
Shore Hardness 27 Shore D ASTM D2240 at 23°C (73°F)
Overlap Shear Strength 2000 lb/in² Etched Aluminum, 7 d cure at 23°C (73°F)
T-Peel Adhesion 35 lb/in ASTM D1876, Etched Aluminum at 23°C (73°F)
Elongation 120 % ASTM D882 at 23°C (73°F)
Tensile Strength 600 lb/in² ASTM D882 at 23°C (73°F)
Thermal Conductivity 0.085 (btu-ft)/(h-ft²-°F) C177 at 110°F
Dielectric Constant 9.2 - ASTM D150, 1 KHz at 23°C (73°F)
Volume Resistivity 1.5E+10 Ohm-cm ASTM D257 at 23°C (73°F)
Glass Transition Temperature (Tg) 15 °C (59°F) Mid-Point

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers