3M CA40H

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M CA40H

Main features

  • Higher-Viscosity Controlled Dispensing
  • EPDM, Vinyl, and Aluminum Bonding
  • Alignment-Friendly Slower Set Time

Product Description

3M™ Scotch-Weld™ Instant Adhesive CA40H is a clear, single-component, high-strength cyanoacrylate adhesive designed for room-temperature curing. Formulated as a higher-viscosity and slightly slower-setting alternative to standard CA40, it helps prevent run-off during application while providing extra time for precise part alignment. This adhesive delivers exceptional performance on difficult-to-bond substrates, offering particularly good adhesion to aluminum, EPDM rubber, and flexible vinyl, alongside good resistance to soap solutions and isopropyl alcohol.

Key features

  • Controlled application: Higher viscosity formulation (400-600 cP) helps prevent adhesive run-off for cleaner, more precise dispensing.
  • Optimized set time: Slightly slower setting time allows for the proper alignment of parts before handling strength is achieved.
  • Difficult substrate bonding: Provides strong, reliable bonds to challenging materials such as aluminum, EPDM rubber, and flexible vinyl.

Applications / Suitable for

  • Bonding difficult-to-bond rubbers, plastics, and metals
  • Assembling EPDM rubber and flexible vinyl components
  • Applications requiring resistance to soap solutions and isopropyl alcohol

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear
Chemistry Type
Ethyl
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
100 ˚C
Physical Properties
Net Weight
87 kg/m3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Ethyl Cyanoacrylate - -
Color Clear - -
Specific Gravity 1.05 - -
Viscosity 400 - 600 cP -
VOC Content <= 6 g/L Less H2O & Exempt Solvents
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Time to Handling Strength 5-40 seconds -
Long Term Temperature Resistance 100 °C (212°F)
Minimum Long Term Temperature Resistance -54 °C (-65°F)