3M AF3028

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M AF3028

Main features

  • Expandable Core Splice Filling
  • Low Sag Cure Behavior
  • Wide Temperature Structural Performance

Product Description

3M Scotch-Weld Structural Core Splice Film AF 3028 is a low-density, expandable epoxy film for filling mismatch areas, reinforcing honeycomb core, and creating core splices. The off-white unsupported film expands during cure to fill the joint while maintaining low sag and low volatile loss. AF 3028 supports cure temperatures from 121 to 176 deg C and provides structural performance from -55 to 176 deg C. Protective liners support cutting and placement before the honeycomb assembly is closed and cured under the selected process conditions.

Key features

  • Expandable Core Splice Filling: The film expands during cure to fill mismatch areas and honeycomb splice joints.
  • Low Sag Cure Behavior: Controlled flow helps the film remain positioned as the assembly heats.
  • Wide Temperature Performance: Cured splice performance covers demanding aerospace temperature conditions.

Applications

Honeycomb core splicing, core reinforcement, mismatch filling, and aerospace sandwich-panel assembly.

Technical Specifications

General Properties
Color
The color
Off White

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BaseEpoxy-As supplied
ColorOff white-As supplied
FormUnsupported film-With protective liners
Nominal thickness50 +/- 5milUncured film
Approximate areal weight0.26lb/ft2AF 3028
Approximate expansion ratio1.9-Uncured characterization
Approximate uncured density63lb/ft3As supplied
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Cured density34lb/ft3Free film; 60 min at 121 deg C; 4 to 6 deg F/min rise
Expansion ratio1.8-Free film; 60 min at 121 deg C; 4 to 6 deg F/min rise
Sag0.8mm90 min at 121 deg C; vertical aluminum panel
Splice delamination strength490N5052 honeycomb core; 60 min at 121 deg C; tested at 24 deg C
Tube shear strength6.5MPaCure Cycle A; tested at 24 deg C