3M AF163-2OST

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AF163-2OST

Main features

  • One Side Tack Layup
  • Nonwoven Carrier Handling
  • Selectable Bondline Construction

Product Description

3M Scotch-Weld Structural Adhesive Film AF 163-2 OST is a modified epoxy structural adhesive film with a matte nonwoven carrier and one-side-tack construction. The differentiated tack surfaces support layup control by providing higher tack on one side and a lower-tack surface on the carrier side. Available AF 163-2 OST weights provide selectable bondline thickness and color for prepared metal, composite, and honeycomb assemblies. The family supports low-pressure and vacuum cure processing. Substrate preparation, primer, pressure, and cure cycle define the complete bonding process.

Key features

  • One Side Tack Construction: Differentiated tack surfaces support controlled film placement during layup.
  • Nonwoven Carrier Support: The matte carrier improves handling before heat cure.
  • Selectable Film Weights: Multiple areal weights provide options for bondline construction.

Applications

Structural bonding of prepared aerospace metals, composites, and honeycomb assemblies where one-side tack supports layup.

Technical Specifications

Other Properties
Storage Temperature
-18 °C
General Properties
Color
The color
Green

Additional Information

Technical properties

As-supplied / before-processing properties

Values are listed by AF 163-2 OST film weight to preserve configuration context.

PropertyValueUnitMethod / condition
ConstructionOne side tack with matte nonwoven carrier-OST designation
Nominal areal weight options0.030; 0.045; 0.060lb/ft2AF 163-2 OST variants
Color by weightGreen; green; red-Corresponding weight variants
Nominal thickness by weight5.5; 5.5; 9.5milCorresponding weight variants

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers