3M AF126-3

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M AF126-3

Main features

  • Low Temperature Cure
  • Controlled Low Flow Processing
  • Green Supported Film Handling

Product Description

3M Scotch-Weld Structural Adhesive Film AF 126-3 is a green, toughened epoxy structural adhesive film for bonding prepared metal, composite, and honeycomb assemblies. Its matte nonwoven scrim-supported construction combines low tack for handling with low flow for bondline control during cure. The film can cure at temperatures as low as 82 deg C, supporting lower-temperature processing where the complete assembly permits it. Metal preparation, primer selection, applied pressure, and the full time-and-temperature cure schedule define the complete bonding process.

Key features

  • Low Temperature Cure: The film can cure at temperatures as low as 82 deg C.
  • Low Flow Bondline Control: Controlled flow helps retain adhesive placement during cure.
  • Green Supported Construction: The matte nonwoven scrim provides handling support during layup.

Applications

Structural bonding of prepared metals, composites, and honeycomb sandwich assemblies.

Technical Specifications

General Properties
Color
The color
Green
Physical Properties
Volatiles
Less than 1 %
Other Properties
Storage Temperature
-18 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Film constructionMatte nonwoven scrim supported-AF 126-3
ColorGreen-As supplied
Nominal areal weight294g/m20.060 lb/ft2
Nominal caliper0.25mm0.010 in
Volatile contentLess than 1%As supplied
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile shear at 24 deg C37.2MPaAverage with EC-2320 primer
Tensile shear at 82 deg C18.8MPa10 min exposure; average with EC-2320 primer
Tensile shear at -55 deg C42.5MPa10 min exposure; average with EC-2320 primer
T-peel at 24 deg C156N/25 mmAverage with EC-2320 primer

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers