3M AC-770-B-2-3

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-770-B-2-3

Main features

  • Low Density Fuselage Sealing
  • Controlled Thixotropic Placement
  • Extended Class B Work Life

Product Description

3M Aerospace Sealant AC-770 Class B-2-3 is a two-part, low-density, manganese-dioxide-cured polysulfide sealant for aircraft fuselage sealing. Its thixotropic Class B paste supports extrusion, injection, and spatula placement while resisting flow after application. The system uses a 100:10 base-to-accelerator mix ratio by weight. Class B schedules include B-1 and B-2 grades, with B-2 providing a 2 hour application life at 77 deg F and 50% relative humidity. After cure, the dark-brown sealant remains flexible across a broad aerospace service temperature range.

Key features

  • Low Density Fuselage Sealing: The cured sealant combines a 1.10 specific gravity with aircraft joint sealing.
  • Thixotropic Application Control: Class B consistency supports extrusion, injection, and spatula placement.
  • Extended B2 Work Life: The B-2 schedule provides a 2 hour application life under controlled conditions.

Applications

Aircraft fuselage joint sealing by extrusion, injection, or spatula application.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Base / Accelerator)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.10
Thermal Properties
Service temperature
-54 to 121 °C
Other Properties
Storage Temperature
Below 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Base colorOff white-Before mixing
Accelerator colorBrown-Before mixing
Mix ratio by weight100:10base:acceleratorClass B system
Nonvolatile content98.5%Typical
Base viscosity9500 to 13000poiseBrookfield RVT, spindle 7, 2 rpm, 77 deg F
B-2 schedule2; 7 to 8; 9 to 11hApplication life; tack-free time; cure time at 77 deg F and 50% relative humidity
Shelf life9monthsStored below 80 deg F
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorDark brown-Cured 14 days at 77 deg F and 50% relative humidity
Specific gravity1.10-Cured
Hardness42 to 48Shore ACured
Tensile strength250psiStandard cure
Elongation310%Standard cure
Service temperature range-54 to 121deg CCured sealant