3M AC-730

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-730

Main features

  • Non Chromated Corrosion Inhibition
  • Flowable And Thixotropic Options
  • Selectable Application Life Grades

Product Description

3M Aerospace Sealant AC-730 is a two-part, non-chromated, corrosion-inhibiting polysulfide sealant family for aircraft faying surfaces and joints. Class B grades are thixotropic pastes for extrusion, injection, or spatula placement, while Class C grades are flowable materials for fay-surface application. Both classes use a 100:10 base-to-accelerator mix ratio by weight. Multiple grade schedules let users select an application-life window for the assembly process. After cure, the sealant provides low-temperature flexibility and service capability from -54 to 121 deg C.

Key features

  • Non Chromated Corrosion Inhibition: The polysulfide system supports protected aircraft sealing without chromate inhibitor.
  • Class B And C Options: Thixotropic and flowable forms address different joint and faying-surface processes.
  • Selectable Application Life: Multiple grade schedules support short or extended assembly windows.

Applications

Aircraft faying-surface and joint sealing using the class and grade matched to the application method.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Base / Accelerator)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.5
Other Properties
Storage Temperature
Below 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Class B and Class C values are separated to preserve their different application forms.

PropertyValueUnitMethod / condition
Mix ratio by weight100:10base:acceleratorClass B and Class C systems
Class B formThixotropic paste-Extrusion, injection, or spatula application
Class B base viscosity9500 to 16000poiseBrookfield RVT, spindle 7, 2 rpm, 25 deg C
Class B nonvolatile content98%Typical
Class C formFlowable-Fay-surface application
Class C base viscosity2000 to 4000poiseBrookfield RVT, spindle 7, 2 rpm, 25 deg C
Class C nonvolatile content90%Typical
Technical properties

After-processing / final-state properties

Final-state values retain their Class B or Class C test context.

PropertyValueUnitMethod / condition
Class B specific gravity1.52-Cured 14 days at 25 deg C and 50% relative humidity
Class C specific gravity1.5-Cured 14 days at 25 deg C and 50% relative humidity
Class B hardness50Shore ACured
Low-temperature flexibilityNo checking or adhesion loss-At -54 deg C
Service temperature range-54 to 121deg CCured sealant
Short-duration temperature range-54 to 182deg CCured sealant

Leading Brands Trust in Our Products and Services