3M AC-130-2

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M AC-130-2

Main features

  • Non Chromated Metal Preparation
  • Ambient Dry Process
  • Brush Spray Or Immersion Application

Product Description

3M Surface Pre-Treatment AC-130-2 is a two-part, water-based, non-chromated sol-gel surface treatment for preparing aluminum alloys, steel, and titanium before adhesive bonding. The mixed treatment can be applied by brush, spray, or immersion and dries at ambient conditions without a rinse or heat-cure step. A 30 minute induction period prepares the mixture for use, followed by a 10 hour pot life. Applying the compatible primer or adhesive within 24 hours of treatment helps maintain the intended bonding process window.

Key features

  • Non Chromated Sol Gel: The water-based treatment prepares compatible metals without a chromate conversion step.
  • Ambient Dry Processing: Brush, spray, or immersion application requires no rinse or heat cure.
  • Flexible Metal Preparation: The treatment supports aluminum alloys, steel, and titanium bonding processes.

Applications

Surface preparation of aluminum alloys, steel, and titanium before compatible adhesive bonding.

Technical Specifications

General Properties
Color
The color
As mixed, it is slightly cloudy un-tinted
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
10 hours
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values describe the mixed treatment before and during application.

PropertyValueUnitMethod / condition
System configurationTwo part-Mix before use
Mixed appearanceSlightly opaque and untinted-After mixing
Induction time30minBefore application
Pot life10hAfter induction
Application temperature14 to 31deg CBrush, spray, or immersion
Maximum relative humidity85%During application and drying
Primer or adhesive window24hAfter treatment