3M 966

Main features

  • Up to 232 deg C Short-Term Exposure
  • 10,000-Minute Static Shear
  • Metal and High-Energy-Plastic Bonding

Product Description

3M™ Adhesive Transfer Tape 966 is a 2.3 mil (0.06 mm) adhesive transfer tape featuring 3M™ High Temperature Acrylic Adhesive 100 on a 62# densified kraft liner. It provides excellent bonding to metals and high-surface-energy plastics, exceptional static shear performance at elevated temperatures, and resistance to demanding chemical and environmental exposure. Its low-outgassing and low-leachable-chloride characteristics make it suitable for evaluated electronic, aerospace, industrial labeling, nameplate, and die-cutting applications.

Key features

  • High-temperature performance: Supports short-term exposure up to 232°C (450°F) and long-term exposure up to 204°C (400°F).
  • Exceptional static shear: Achieves 10,000-minute static shear results at temperatures from 23 to 232°C under the published test conditions.
  • Strong high-surface-energy bonding: Provides excellent adhesion to metals and good adhesion to high-surface-energy plastics.
  • Environmental and chemical resistance: Resists humidity, water, UV exposure, temperature cycling, gasoline, oil, mild acids, and mild alkalis when properly applied.
  • Low-outgassing construction: Offers low outgassing and low leachable chloride for evaluated electronic and aerospace applications.

Applications / Suitable for

  • Bonding metal nameplates
  • High-temperature labels and identification components
  • Die-cut parts requiring a densified kraft liner
  • Evaluated electronic, aerospace, and industrial applications

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
acrylic
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
62# Densified Kraft with “3M” printed in green
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
60 μm

Additional Information

Technical properties

As-supplied / before-processing properties

Representative or typical product properties. Values should not be used for specification purposes.

Property Value Unit Method / condition
Adhesive type 3M™ High Temperature Acrylic Adhesive 100 — Pressure-sensitive acrylic adhesive
Total tape thickness 0.06 (2.3) mm (mil) ASTM D3652
Liner 62# densified kraft with “3M” printed in green — As supplied
Liner thickness 0.09 (3.6) mm (mil) Published typical value
90° peel adhesion — ABS 4.8 (44); 5.9 (54) N/cm (oz/in) ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — stainless steel 5.8 (53); 8.5 (78) N/cm (oz/in) ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil PET backing at 20 min and 2 mil aluminum-foil backing at 72 h; 304 mm/min (12 in/min)
Static shear — 23°C (73°F) 10,000 minutes ASTM D3654; 2,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 70°C (158°F) 10,000 minutes ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 93°C (200°F) 10,000 minutes ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Static shear — 232°C (450°F) 10,000 minutes ASTM D3654; 400 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes
Short-term temperature resistance 232 (450) °C (°F) Short term: minutes or hours
Long-term temperature resistance 204 (400) °C (°F) Long term: days or weeks
Low-temperature service -40 (-40) °C (°F) Parts should be tested for low-temperature shock service
Thermal conductivity 0.178; 0.183; 0.187 W/m/K ASTM C518; at 41°C (107°F), 71°C (160°F), and 101°C (214°F), respectively
Dielectric constant 2.92 — ASTM D150; 23°C (73°F); 1 kHz
Dissipation factor 0.025 — ASTM D150; 23°C (73°F); 1 kHz
Dielectric strength 1,100 V/mil ASTM D149; 500 VAC RMS; 60 Hz/sec
Volume resistivity 4 × 1015 Ω·cm ASTM D257; 23°C (73°F)
Application temperature range 21 to 38 (70 to 100) °C (°F) Ideal range; application below 10°C (50°F) is not recommended for most pressure-sensitive adhesives
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in a sealed plastic bag and out of direct sunlight