3M 950

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 950

Main features

  • 5 mil Adhesive 300 Construction
  • High Initial Adhesion and Holding
  • Multi-Substrate Pressure-Sensitive Bonding

Product Description

3M™ Adhesive Transfer Tape 950 is a 5 mil (0.13 mm) adhesive transfer tape featuring 3M™ Adhesive 300, a pressure-sensitive, medium-firm, fibered acrylic adhesive supplied on a tan 60# glassine liner. It provides very high initial adhesion with good holding power across a range of materials, including metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.

Key features

  • High initial adhesion: 3M™ Adhesive 300 provides strong initial bonding with good holding power.
  • Broad substrate compatibility: Bonds to metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
  • Conformable 5 mil adhesive: The 0.13 mm adhesive thickness supports bonding to surfaces where texture may be visible.
  • Environmental resistance: Provides resistance to humidity, water, UV exposure, temperature cycling, oil, mild acids, and mild alkalis when properly applied.
  • UL-recognized construction: Recognized under UL 969 for Marking and Labeling Systems Materials Components.

Applications / Suitable for

  • Bonding graphic nameplates and overlays
  • Attaching metal nameplates and rating plates
  • Laminating foam for gasket applications
  • Joining similar and dissimilar industrial materials

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
300 Fibered Acrylic
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Tan 60# Glassine
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
130 μm

Additional Information

Technical properties

As-supplied / before-processing properties

Representative or typical product properties. Values should not be used for specification purposes.

Property Value Unit Method / condition
Adhesive type 3M™ Adhesive 300, fibered acrylic — Pressure-sensitive, medium-firm acrylic
Total tape thickness 0.13 (5) mm (mil) ASTM D3652
Liner 60# glassine — Tan primary liner
Liner thickness 0.08 (3.2) mm (mil) Published typical value
90° peel adhesion — ABS 3.7 (34); 4.4 (40) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — polypropylene 6.6 (60); 6.8 (62) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — stainless steel 8.1 (74); 9.4 (86) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
Short-term temperature resistance 121 (250) °C (°F) Short term: minutes or hours
Long-term temperature resistance 70 (158) °C (°F) Long term: days or weeks
Lower temperature service limit -40 (-40) °C (°F) Properly applied tape
Coefficient of thermal expansion — first heat 20 × 10-5 m/m/°C ASTM D696
Coefficient of thermal expansion — second heat 58 × 10-5 m/m/°C ASTM D696
Dielectric constant 3.21 — ASTM D150; 23°C (73°F); 1 kHz
Dissipation factor 0.04 — 23°C (73°F); 1 kHz
Dielectric strength 340 V/mil ASTM D149; 500 VAC RMS, 60 Hz/sec
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight