3M 9379

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 9379

Main features

  • Thin Profile Transfer Bonding
  • Clear Low Visibility Construction
  • Fuel And Hydraulic Fluid Resistance

Product Description

3M Adhesive Transfer Tape 9379 is a clear specialty acrylic transfer adhesive supplied on a clear polyester release liner. The approximately 1.7 mil adhesive layer is designed for environmental sealing and bonding where a thin, conformable adhesive is preferred. It supports impervious aluminum-to-aluminum assemblies exposed to demanding fluids and temperatures when prepared and laminated under the specified conditions. A clear construction keeps the bondline unobtrusive, while the removable liner protects the adhesive during converting and placement. Roll width and length can be selected for the intended production format.

Key features

  • Thin Transfer Adhesive: The approximately 1.7 mil adhesive layer supports low-profile bonding and sealing.
  • Clear Bondline Construction: Clear adhesive and liner simplify placement where appearance matters.
  • Fluid Resistant Bonding: Qualified aluminum bonds resist JP-4 jet fuel and Skydrol hydraulic fluid exposure.

Applications

Environmental sealing and bonding of impervious aluminum assemblies, including converted parts that require a thin transfer adhesive.

Technical Specifications

Other Properties
Storage Temperature
Maximum 26.67 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Adhesive typeSpecialty acrylic-As supplied
Adhesive thicknessApproximately 1.7milBefore lamination
Adhesive colorClear-As supplied
Release linerClear polyester-Removable liner
Shelf life24monthsStored at 80 deg F maximum
Conditioning time24hEquilibrate before lamination
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Short-duration temperature limit450deg FBonded assembly
Long-duration temperature limit300deg FBonded assembly
Low-temperature limit-40deg FBonded assembly
Chemical resistanceJP-4 jet fuel and Skydrol hydraulic fluid-Impervious aluminum bonded to aluminum