3M 9082

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 9082

Main features

  • 177 deg C Long-Term Bonding
  • Low-Outgassing Electronics Adhesion
  • Thin 0.05 mm Transfer Layer

Product Description

3M Ultra High Temperature Adhesive Transfer Tape 9082 is a clear 0.05 mm acrylic adhesive transfer tape with a 0.08 mm 55# densified-kraft release liner for thin, high-temperature bonding in electronics and automotive assemblies. The low-outgassing adhesive system retains measurable adhesion through elevated-temperature testing: 180 deg peel adhesion is 8.8 N/cm at 23 deg C and 5.3 N/cm at 177 deg C on aluminum-foil-backed specimens. Long-term temperature resistance is 177 deg C and short-term resistance is 280 deg C. The construction is intended for assemblies that combine thin bondlines with elevated processing or operating temperatures.

Key features

  • High-temperature acrylic bonding: Long-term temperature resistance reaches 177 deg C, with short-term exposure resistance to 280 deg C.
  • Low-outgassing thin transfer layer: The clear 0.05 mm adhesive layer provides a thin bonding profile for electronics and automotive assemblies.
  • Measured elevated-temperature adhesion: Peel adhesion remains measurable through 230 deg C testing, with 5.3 N/cm recorded at 177 deg C.

Applications

Applications include automotive under-hood bonding, flexible printed circuit and FR-4 attachment, electronics and heat-sink bonding, and solder-reflow process assemblies.

Technical Specifications

General Properties
Color
The color
Clear | White, with green “3M” print
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
50 μm
Other Properties
Storage Temperature
16 - 27 °C
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.16 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorClearAs supplied
Density0.98g/cm^3Typical
Adhesive typeAcrylic adhesive systemHigh-temperature adhesive
Adhesive thickness0.05mmASTM D3652; typical
Liner55# densified kraftWhite with green 3M print
Liner thickness0.08mmTypical
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion at 23 deg C8.8N/cmASTM D3330; 2 mil aluminum foil backing; typical
180 deg peel adhesion at 177 deg C5.3N/cmASTM D3330; specimen conditioned 2 min at temperature; typical
Overlap shear strength at 23 deg C620kPaASTM D1002 / ISO 4587; stainless steel; typical
Long-term temperature resistance177deg CDays to weeks; typical
Short-term temperature resistance280deg CMinutes to hour; typical
Dielectric strength at 23 deg C1200VASTM D149; typical