3M 8992L

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8992L

Main features

  • Linered Die-Cut Masking Format
  • High-Temperature Silicone Masking
  • Clean One-Piece Process Removal

Product Description

3M Polyester Tape 8992L is the linered version of 3M Polyester Tape 8992, combining a 0.052 mm dark-green polyester backing, silicone pressure-sensitive adhesive, and 0.075 mm polyester release liner for die cutting and converting. The tape is 0.082 mm thick excluding the liner and performs from -50 to 204 deg C. Typical data include 48 N/100 mm adhesion to steel, 998 N/100 mm tensile strength, and 148% elongation. Its thermal and chemical resistance support high-temperature masking, while the strong backing removes in one piece and leaves a sharp paint line.

Key features

  • Linered conversion format: The 0.075 mm polyester liner supports die cutting and converted masking shapes before application.
  • High-temperature silicone masking: Silicone adhesive performs from -50 to 204 deg C for powder coating and other elevated-temperature processes.
  • Strong clean process removal: High tensile strength supports one-piece removal without slivering after demanding masking operations.

Applications

Applications include high-temperature powder-coat masking, die cutting and converting, chemical milling, composite vacuum-bag holding, flash breaking, and scratch protection.

Product Family

3M 8992L

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Green
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
82 μm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
148 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
99.8 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyesterDark green
AdhesiveSiliconePressure-sensitive
Backing thickness0.052mmASTM D3652; typical
Total tape thickness0.082mmExcludes liner; ASTM D3652; typical
Liner thickness0.075mmPolyester liner; ASTM D3652; typical
Shelf life24monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion to steel48N/100 mmASTM D3330; typical
Tensile strength998N/100 mmASTM D3759; typical
Elongation at break148%ASTM D3759; typical
Temperature use range-50 to 204deg COperating range

Leading Brands Trust in Our Products and Services