3M 8934

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8934

Main features

  • Glass-Reinforced Packaging Strength
  • Minimal-Rubdown Package Reinforcement
  • Transparent Reinforcement Preserves Graphics

Product Description

Tartan Filament Tape 8934 is a clear glass-yarn reinforced BOPP tape with pressure-sensitive synthetic rubber-resin adhesive for light-duty strapping and package reinforcement. The 0.102 mm construction combines good initial adhesion with high tensile and shear strength, while the transparent backing keeps box graphics and printing visible. Typical performance includes 53 N/100 mm 180 deg peel adhesion to stainless steel after 72 hours at 23 deg C, 3% elongation at break, and 175.1 N/cm tensile strength. Application is easiest at room temperature.

Key features

  • Glass-yarn tensile reinforcement: Glass yarn filaments add tensile strength for box closing, bundling, reinforcing, and pallet unitizing.
  • Low-rubdown initial adhesion: Synthetic rubber-resin adhesive develops good initial adhesion and holds with minimal rub-down on common packaging surfaces.
  • Transparent protective backing: Clear BOPP construction keeps graphics visible while resisting nicks, abrasion, moisture, and scuffing.

Applications

Applications include box closing and reinforcement, light-duty strapping, bundling, sealing, palletizing, and intra-plant movement of packaged goods.

Technical Specifications

General Properties
Color
The color
Clear
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
3 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
175.1 N/cm
Other Properties
Storage Temperature
4 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Adhesive typePressure-sensitive synthetic rubber-resinAs supplied
BackingBiaxially oriented polypropylene (BOPP)Clear backing
Fiber reinforcementGlass yarnAs supplied
Total tape thickness0.102mmASTM D3652; typical
Shelf life18monthsOriginal packaging; 4 to 27 deg C and 40 to 50% RH
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion53N/100 mmASTM D3330; stainless steel; 72 h dwell; 23 deg C; typical
Elongation at break3%ASTM D3759; typical
Tensile strength175.1N/cmASTM D3759; typical

Leading Brands Trust in Our Products and Services