3M 890

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 890

Main features

  • High-Strength Filament Reinforcement
  • Heavy-Duty Bundling Support
  • Industrial Splicing and Securing

Product Description

Scotch Filament Tape 890 is a high-strength glass-filament reinforced polyester tape for heavy-duty bundling, reinforcing, splicing, and securing. Its reinforced construction is used where grouped materials require a high-strength tape wrap during industrial handling, packaging, or transport. The same product supports heavy-duty splicing and component-securing work without changing tape type. The product is intended for heavy-duty industrial packaging and handling tasks. It is available in multiple widths and roll lengths for different roll-format requirements.

Key features

  • High-strength filament reinforcement: Glass-filament reinforced construction provides the strength needed for demanding bundling and securing tasks.
  • Heavy-duty bundling use: The tape is used to bundle pipes, rods, conduit, and timber during industrial handling.
  • Industrial splicing and securing: The product supports heavy-duty paper splicing and secures appliance and furniture lift flaps.

Applications

Scotch Filament Tape 890 is used for heavy-duty bundling of pipes, rods, conduit, and timber, heavy-duty paper splicing, and securing appliance and furniture lift flaps.

Technical Specifications

General Properties
Color
The color
Clear or Black
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
200 μm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
8 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
1380 N/cm
Other Properties
Storage Temperature
4 - 27 °C