3M 8681HS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8681HS

Main features

  • Polyurethane Leading-Edge Erosion Protection
  • Conformable Curved-Surface Coverage
  • High-Shear Acrylic Attachment

Product Description

3M Polyurethane Protective Tape 8681HS is a leading-edge erosion-protection tape built with an abrasion-resistant polyurethane elastomer backing, a high-shear pressure-sensitive acrylic adhesive, and an easy-release plastic liner. The polyurethane resists puncture, tearing, abrasion, erosion, and ultraviolet exposure while remaining conformable over curved surfaces. Typical data include 500% elongation at break, 148 N/100 mm peel adhesion to bare aluminum at 21 deg C, and a maximum service temperature of 82 deg C. The tape can be painted or applied over painted surfaces and is designed for protective coverage on exposed leading-edge surfaces.

Key features

  • Erosion-resistant polyurethane: Tough polyurethane construction resists puncture, tearing, abrasion, and erosion on exposed leading edges.
  • Conformable curved-surface application: The tape follows curved surfaces for protective coverage on rotor blades and other leading-edge geometries.
  • High-shear acrylic attachment: A long-aging, solvent-resistant acrylic adhesive provides pressure-sensitive attachment for demanding surface-protection use.

Applications

Applications include rotor-blade, aircraft, and industrial leading-edge protection in areas exposed to abrasion, erosion, rain, or sand.

Product Family

3M 8681HS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
1,540 N/cm
Thermal Properties
Operating Temperature
82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Polyurethane film thickness0.30mmApproximate applied film thickness; typical
Acrylic adhesive thickness0.06mmApproximate applied adhesive thickness; typical
LinerEasy-release plasticSkip-slit or non-skip-slit configurations
Standard roll length32.9m36 yd; typical
Shelf life2yearsFrom date of manufacture or as expressly certified by 3M
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Elongation at break500%ASTM D882; typical
Peel adhesion to bare aluminum148N/100 mmASTM D3330; 21 deg C; typical
Peel adhesion to ABS plastic60N/100 mmASTM D3330; 21 deg C; typical
Maximum service temperature82deg CTypical