3M 8672

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8672

Main features

  • UV-Resistant Outdoor Surface Protection
  • 8-Mil Conformable Erosion Barrier
  • High-Peel Acrylic Surface Adhesion

Product Description

3M Polyurethane Protective Tape 8672 is an 8 mil outdoor-grade polyurethane tape with acrylic pressure-sensitive adhesive and a polyester liner for leading-edge erosion and abrasion protection. The 6 mil polyurethane film is formulated for ultraviolet resistance and resists puncture, tearing, abrasion, and erosion, while the thin construction conforms over curved surfaces. The tape can be painted or applied over painted surfaces, and its acrylic adhesive provides high peel strength on tested aluminum, acrylic enamel, and ABS surfaces. It is designed for aircraft production and maintenance and other aerospace or industrial surfaces exposed to outdoor wear, including rain and sand erosion.

Key features

  • UV-resistant outdoor polyurethane: The protective film is formulated for ultraviolet exposure and resists puncture, tearing, abrasion, and erosion in outdoor service.
  • Thin conformable construction: The 8 mil total tape thickness follows curved surfaces while providing a durable leading-edge protective layer.
  • High-peel acrylic adhesion: The acrylic adhesive provides measured peel adhesion on bare aluminum, acrylic enamel, and ABS while retaining a pressure-sensitive format.

Applications

Use 3M Polyurethane Protective Tape 8672 for leading-edge, erosion, scratch, and abrasion protection on aerospace and industrial surfaces, including painted or curved areas.

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
700 N/cm
Thermal Properties
Operating Temperature
82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Film materialPolyurethaneOutdoor-grade protective film
Film thickness0.006in0.15 mm
AdhesiveAcrylic pressure-sensitive adhesiveProduct construction
Adhesive thickness0.002in0.06 mm
LinerPolyesterEasy-release liner
Tensile strength at break40lb/inTypical; 700 N/100 mm; ASTM D882
Elongation at break500%Typical; ASTM D882
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Approximate applied thickness0.008in0.21 mm; film plus adhesive; liner excluded
Peel adhesion to bare aluminum60oz/inTypical; 66 N/100 mm; ASTM D1000 at 21 deg C
Peel adhesion to acrylic enamel43oz/inTypical; 48 N/100 mm; ASTM D1000 at 21 deg C
Peel adhesion to ABS plastic50oz/inTypical; 55 N/100 mm; ASTM D1000 at 21 deg C
Maximum service temperature180deg F82 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers