3M 8671

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8671

Main features

  • Outdoor UV-Resistant Edge Protection
  • Acrylic Pressure-Sensitive Protective Layer
  • Converted Formats for Leading Edges

Product Description

3M Polyurethane Protective Tape 8671 is an outdoor- and UV-resistant polyurethane protective tape with acrylic pressure-sensitive adhesive and a liner for leading-edge abrasion and erosion protection. The polyurethane film provides a protective surface layer for aerospace and industrial exposure, and the pressure-sensitive construction is supplied in multiple widths, lengths, and converted shapes. Its outdoor and ultraviolet resistance make the tape appropriate for exposed leading-edge service. The product is used on aircraft, rotor blades, and industrial leading edges where abrasion and erosion protection are required under outdoor operating conditions.

Key features

  • Outdoor and UV resistance: The polyurethane film is designed for outdoor and ultraviolet exposure in leading-edge protection applications.
  • Acrylic pressure-sensitive construction: The acrylic adhesive provides a pressure-sensitive protective-tape format for direct surface application.
  • Configurable protective formats: Multiple widths, lengths, and converted shapes support application to aircraft, rotor-blade, and industrial leading-edge geometries.

Applications

Use 3M Polyurethane Protective Tape 8671 for aircraft, rotor-blade, and industrial leading-edge protection where outdoor abrasion and erosion exposure must be managed.

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Thermal Properties
Service temperature
Maximum 82 °C