3M 8657DL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 8657DL

Main features

  • Dual-Liner Aircraft Wet-Area Installation
  • Tough Polyurethane Fluid-Barrier Protection
  • 82 deg C Wet-Area Service

Product Description

3M Polyurethane Protective Tape 8657DL is a flame-retardant dual-liner polyurethane protective tape for wet-area corrosion prevention in aircraft interiors. The tough polyurethane elastomer resists puncture, tearing, abrasion, and scratching, while the pressure-sensitive adhesive provides straightforward attachment over aircraft floor panels. A 3 mil polyethylene bottom liner protects the adhesive before application, and a 2 mil polyester top liner serves as an installation aid before final removal. Installed over floor panels and adjoining walls, the tape forms a fluid barrier for areas such as lavatories and galleys. Its approximate applied thickness is 0.46 mm, with a maximum service temperature of 82 deg C.

Key features

  • Dual-liner installation control: The 3 mil polyethylene bottom liner and 2 mil polyester top liner protect the adhesive and aid controlled installation.
  • Tough polyurethane fluid barrier: The flame-retardant polyurethane elastomer resists puncture, tearing, abrasion, and scratching in aircraft wet areas.
  • Wet-area service capability: The installed tape forms a fluid barrier over floor panels and has a maximum service temperature of 82 deg C.

Applications

Use 3M Polyurethane Protective Tape 8657DL over aircraft floor panels and adjoining walls in wet areas such as lavatories and galleys to limit fluid exposure to the floor system.

Product Family

3M 8657DL

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
600 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
1540 N/cm
Thermal Properties
Operating Temperature
82 °C
General Properties
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
460 μm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolyurethane elastomerFlame-retardant tape construction
AdhesivePressure-sensitive adhesiveProduct construction
Bottom liner thickness3milPolyethylene liner
Top liner thickness2milPolyester application-aid liner
Tensile strength88lb/inTypical; 1540 N/100 mm; ASTM D882 Method A
Elongation at break600%Typical; ASTM D882 Method A
Hardness90Shore ATypical; ASTM D2240
Shelf life2yearsFrom date of manufacture; stored clean, dry, and out of direct sunlight
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Approximate applied thickness0.018in0.46 mm; liner excluded
Peel adhesion to bare aluminum35oz/inTypical; 38 N/100 mm; ASTM D3330 180 deg peel; 24 hr dwell on 2024-T3 aluminum
Peel adhesion to BMS 4-17 Type VI floor panel19oz/inTypical; 21 N/100 mm; ASTM D3330 180 deg peel; 24 hr dwell
Peel adhesion to BMS 4-20 Type II floor panel23oz/inTypical; 25 N/100 mm; ASTM D3330 180 deg peel; 24 hr dwell
Maximum service temperature180deg F82 deg C