3M 855

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 855

Main features

  • Clean-Removal High-Temperature Masking
  • Non-Silicone Adhesive for Repainting
  • High-Elongation Composite Bagging Tape

Product Description

3M High Temperature Nylon Film Tape 855 is a 3.6 mil nylon film tape with a non-silicone rubber pressure-sensitive adhesive for high-temperature masking, composite bagging, and metal bonding operations. The tough 2.0 mil nylon backing has 460% elongation for conformable masking and quick removal around process surfaces. Tape 534.375removes cleanly after several hours at 350 deg F (177 deg C) and supports shorter bake cycles up to 400 deg F (204 deg C). Its non-silicone adhesive avoids silicone residue that can interfere with subsequent painting or bonding, making the tape useful for autoclave hold-down, masking, and flash-removal steps.

Key features

  • Non-silicone high-temperature adhesive: The rubber adhesive removes cleanly after high-temperature exposure without leaving silicone residue before later painting or bonding.
  • High-elongation nylon backing: The 460% elongation nylon film conforms during masking and facilitates quick, efficient removal after processing.
  • Short-cycle bake capability: The tape withstands several hours at 350 deg F and shorter bake cycles up to 400 deg F for composite and metal-bond processing.

Applications

Use 3M High Temperature Nylon Film Tape 855 to hold composite or metal bonding materials during autoclave processing, mask advanced composite and metal bonds, and assist flash removal after bonding.

Technical Specifications

General Properties
Color
The color
Cream
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
460 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
56 N/cm
Other Properties
Storage Temperature
16 - 27 °C
Thermal Properties
Temperature Range
16 - 204 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingNylonProduct construction
AdhesiveRubberNon-silicone pressure-sensitive adhesive
Backing thickness2.0milTypical; 0.051 mm; ASTM D3652
Total thickness3.6milTypical; 0.091 mm; ASTM D3652
Tensile strength at break32lb/in widthTypical; 560 N/100 mm; ASTM D3759
Elongation at break460%Typical; ASTM D3759
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion to steel57oz/in widthTypical; 61 N/100 mm; ASTM D3330
Clean-removal exposure350deg FAfter several hours; 177 deg C
Short bake-cycle exposure400deg FShort cycles; 204 deg C

Leading Brands Trust in Our Products and Services