3M 853

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 853

Main features

  • 0.06 mm Thin Tape Construction
  • Solvent-Resistant Tape Adhesive
  • Transparent Label-Protection Tape

Product Description

3M™ Polyester Tape 853 is a transparent polyester film tape with a high-shear, solvent-resistant acrylic adhesive. Its thin, high-strength construction provides reliable bonding without obscuring protected information, making it suitable for high-tension splicing, critical label protection, tape hinges, and moisture-sealing applications. The tape withstands long-term temperatures from -50 to 150°C (-60 to 300°F) and resists solvents including jet engine fuel, hydraulic fluid, and lubricating oils.

Key features

  • Thin, strong construction: Combines a 0.03 mm (1.1 mil) polyester backing with a total tape thickness of 0.06 mm (2.2 mil).
  • Solvent-resistant adhesion: Acrylic adhesive resists many solvents, including jet engine fuel, hydraulic fluid, and lubricating oils.
  • Transparent protection: Allows information beneath the tape to remain visible during label-protection and sealing applications.
  • Broad temperature resistance: Supports long-term use from -50 to 150°C (-60 to 300°F).
  • Aerospace flammability performance: Meets FAR 25.853(a), Appendix F, Part I (a)(1)(ii), and can be qualified to Federal Specification L-T-100 Type I.

Applications / Suitable for

  • High-tension splicing
  • Critical label protection
  • Tape hinges
  • Aerospace applications requiring FAR flammability performance
  • Sealing critical areas against moisture intrusion

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
acrylic
Color
The color
transparent
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.03 mm
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
60 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
46 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
83 %
Thermal Properties
Operating Temperature
50 - 150 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Representative or typical product properties. Values should not be used for specification purposes.

Property Value Unit Method / condition
Product construction Polyester backing with acrylic adhesive — As supplied
Color Transparent — As supplied
Backing thickness 0.03 (1.1) mm (mil) ASTM D3652
Total tape thickness 0.06 (2.2) mm (mil) ASTM D3652
180° peel adhesion 5 (46) N/cm (oz/in) ASTM D3330; 23°C (73°F); 304 mm/min (12 in/min)
Tensile strength 43.4 (25) N/cm (lb/in) ASTM D3759
Elongation at break 83 % ASTM D3759
Water vapor transmission 15.5 (1) g/m²/24 h (g/100 in²/24 h) ASTM D3833
Minimum long-term temperature resistance -50 (-60) °C (°F) Long term: days or weeks
Maximum long-term temperature resistance 150 (300) °C (°F) Long term: days or weeks
Standard roll length 65.8 (72) m (yd) Published standard size
Shelf life 18 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight

Leading Brands Trust in Our Products and Services